Madam Steph

I love those lentils, Rase.

I also posted these on the Monthly Colour Challenge:



It's my first go at sugared beads. I made them with Vicki Veebees frit. For those who make them, should I have flashed them through the flame a tad less and left them more 'sugary'?

Linda xxx

Brink Beads

#781


Not sure what happened, lost my last post....



and now for those flowers again :-)


Sara

www.brinkbeads.co.uk

Galloway Beads

Lots of gorgeousness on here again this week. Madeline your Goddess is wonderful. ;D

Some plum puds from me...........just need some brandy sauce  ;D


Plum Puddings by Galloway Beads, on Flickr

Elaine x

www.gallowaybeads.co.uk
My Etsy http://www.etsy.com/shop/Gallowaybeads

Chameleon

Thanks Everyone for the comments on my ring toppers  ;D

Lakelady, looks like you are enjoying trying sculptural beads 
Lovely Autumnal lentils Rase
Linda, I love those sugared beads, they look so frosty and gorgeous
Beautiful flowers Sara, and love the colour combo
nice colours in that plum set Elaine.

Made myself a pendant. Technically its a prototype as I have been asked to make some of these but this one is definitely a keeper  ;D with pmc, fine silver and sterling.


tomcat

made these this morning, for those that know Cornwall, the Lizard, my inspiration was a fabulous mineral found there called Serpentine, its very variable - greens reds into blues with a grey, green brown base. I have bits of it in all shades at home and love it


Mark - Blog - http://beadsbeerandphotos.blogspot.co.uk/
Life is not a game - its THE game, so play it like you mean it
A Long time ago in Egypt cats were worshipped as Gods, cats have not forgotten this !

Kathy

My Trouty friend has now shown me how to upload photos (thank you Trout :-*) So, here is a photo of a bead I made yesterday. I spent a fab day with the very lovely Helen G a couple of weeks ago and have been practising floral beads in a hope to one day be as good as Helen is! I wasn't sure if it would work in these colours but wanted it to go with an outfit so went for it, and was rather pleased with the outcome :D More practice is def. required as there are a couple of bubbles in my encasing and the flowers are FAR from perfect so..........P P P!


DSCF4248 by gameoldbird, on Flickr

Magpie

I don't get to post here as often as I'd like, but each and every week your beads really blow me away.

And I'm sorry, it's all or nothing for me at the moment, no torching for about 3 weeks and suddenly I get 3 goes on the torch in one week. So please excuse the hog.

Pizza Express, recycled goddess beads. by HelenPetersBeads, on Flickr
Goddesses made from a broken water glass from pizza express (full story over on FB if you're interested).


Green BHB by HelenPetersBeads, on Flickr
Silver core bead featuring some of Elaine's murrini that I got in the murrini swap.


Mine, all mine by HelenPetersBeads, on Flickr
Made with colours to match a particular top of mine, just need making up into jewellery.


Liam's beads. by HelenPetersBeads, on Flickr
My nephew had a baby, or his partner did, so I put little Liam's name and birthdate onto BHBs, all I need to do is remember to take them over.


Clear glass with pink frit mix on top. by HelenPetersBeads, on Flickr
More fritty breads.


Decorated recycled black sprees by HelenPetersBeads, on Flickr
More recycled beads.

Thanks for looking.

Amber

No new gallery yet? OK, I'll start  :)

Even more sparkly and shiny in person...Effetre black silver foil and MCD frit.



And I love this one; just white and SIS.



SueP

Beautiful start to the week I have something similar to the first one to show so off for a look ;D

Editted (2 t's??) to add


Earth 2011 (1) by Blue Flame Beads, on Flickr

first time with flickr rather than photobucket so not surewhether will upload ;D ;D ok there now but can I resize here or on flickr ???

Fruddy

Superb start again guys..... Lakelady - love the little jellyfish!  I have that Tut but not even tried to attempt making one of those!

More of the same from me......






suzielaws


LampyLou

It's just as well the boys are at school/nursery, every time I look in here I think, "Oooh, I wonder if I could..?" and I rush back out to my torch and try again. 

A couple of pictures of yesterday's work.  Aren't we lucky to have a sunny day today!


Autumn Glow 1 by Skarda Glass, on Flickr


Grey Day by Skarda Glass, on Flickr

I adore Kaz's lentils, they are fantastic and the BHB have been stunning too.  Thank you for sharing everybody.

Julia x

Helen G

Lovely work everyone, can't wait for the week to unfold if this is anything to go by!

I feel I am finally getting somewhere with "organic" beads.


IMG_4335 by Helen G Beads, on Flickr


IMG_4332 by Helen G Beads, on Flickr

And made some buttons for the first time in a while


IMG_4358 by Helen G Beads, on Flickr


IMG_4359 by Helen G Beads, on Flickr

Ilona

I haven't had chance to look at this thread yet, but will do tomorrow.
Here is a set I made before I went on holiday.