Galloway Beads

Gorgeous start to this weeks thread. :o
I have had a go with clio.




www.gallowaybeads.co.uk
My Etsy http://www.etsy.com/shop/Gallowaybeads

Ilona

#196
Beautiful beads again this week.

I have been trying to brighten things up a bit and made these :)




This last set I am pleased with.



SueP

This S&T just gets better and better :) I especially love the vessel
I've been playing with my heart press:


and some mystic polka dots

MyPrecious

#198
I love the second set too! ;D

Here's a photo of my biggest set ever! I don't know if anyone will buy it but it was fun to make. ;D



And another photo of the same set :


It has 27 beads in it, not counting the spacers!
Kathy

My website

Karen

love those hearts Julie did you use a press?


I actually made beads :)
Karen




Stupid people shouldn't breed, but they DO!!

sublimekate

#200
Been practicing hollows which I've never really been able to get to grips with but something clicked this week. I don't know where I'm going with this, but I am going  :) Coz I really like making them, I'm not sure I've quite got it right but I'm really enjoying making these  :) Kaz's Murrini btw  ;)

So here they are, murrini encrusted hollows, but should I etch them ??? ???

I really want to but they took me so long to make I don't want to ruin them, I've done a test bead so you can see what it would look like....

Honest Opinions please. Kate xxx



Some more  :)

soulsilver

A few new bits from me this week!  Loving everything on here so far, these just keep getting better and better







Ciel

#202
So many lovely beadies so far!

Here are some leaves I've been working on recently :D  (same set - different backgrounds/lighting)




Kalorlo

Here's what I was doing last week:

CiM spacers with my sample pack


Faux boro


Two faux boro tries - the first is by melting in iris gold frit to a straw yellow rod and winding on directly then encasing, the second is a clear core with a straw yellow with iris gold stringer wound on top, then encased. (You can see some blues if you look at it side-on in person). I was wondering if that would cut down on the cola colour - not so much!

Opalinos and turquoise


Dark turquoise with black stringer - the diamond might need an encounter with some toilet cleaner  :P. Then we have carnelian, periwinkle and nile green opalinos. Pretty colours!

Flamingo


Light grey trans core, shaped into an oval with diagonal lines of black, anise white and carnelian opalino added, gravity swirled, reshaped and mashed. I'm rather pleased with these  ;D

dinah46

Well, as I haven't got my heart press at the moment and am holding a grooved marver ransom for it ;D these are what came out of the kiln this morning. I forgot to take a photo before making them up though ::)


SilverGems89

ok here's my offering from today, my very first (and second) goddess beads!
This is the first one, yes she is as tiny as she looks, only 13mm tall!

And the second one, which im so sooooo happy with! she's a bit bigger

Made them with the guidance of teresa laliberte's tutorial, which is fab!
Sorry for the poor pictures, i had to snap them really quick on the kitchen windowsil before it got too dark!

Trudi

great beads everyone. And that second Goddess has really come on!

Another vessel  - a plainish one - but it has mica powder at the bottom and black nebula rim and handles!


Dee Dee

The black nebula vessel is fab Trudi and I particularly like your second set Sally!

A couple of bits from me......

Some Psyche nuggets....



And some frittie beads....


sublimekate

Amazing S&T, I'm jumping in late the list of beautiful work it huge, all gorgeous.

Lampwork has come up trumps and satisfied my rather OCD like personality, I decided PPP as in order on the hollow front, now I'm obsessed with hollows  ;D  ;D Just keep making them, gradually working my way through the transparent shelf   :D So satisfying  :)








There's more but I'm hogging now  ::)

Hazer

I'm here to give you all an ego boost :D

This is about my 9th go at lampworking.

Fritties (frit supplied by June ;D)


LtoR
Accidentally bumpy bead (the gas froze whilst I was melting in dots), Raked dots bead, bead with bead release accents, dotty bead, and plain bead:


Don't they almost look like beads?  :P ;D
ContinuumDesigns- artisan polymer clay beads for one-of-a-kind designs.

The FHFTeam - featuring glass, jewellery and art handmade in the UK.