Silvered stringers?

Started by Kimster, March 02, 2013, 01:05:49 PM

Previous topic - Next topic

0 Members and 3 Guests are viewing this topic.

Kimster

Sorry if this question is a dumb one  :-[  ... I'm just wondering if it's possible to get the same effects of DH glass by making stringers from silver foil/leaf & various transparent glass, then using them in the same way (cooling/heating sequence etc). Or are they manufactured in a totally different way, with very different glass etc? Just asking!

JKC

I have used lots of different colours of stringers and shards with silver leaf and foil and the effects are quite different to DH silver glass, but still pretty. Janet

Margram

What a good question! You'll have to experiment and show the results :)
Marg x  Etsy Flickr My blog

Trudi

Try silver with dark transparent glass like cobalt, dark purple or a deep green - you'll get some nice effects!