Main Menu

gallery archive 11

Started by MangoBeads, January 03, 2011, 05:22:04 PM

Previous topic - Next topic

0 Members and 3 Guests are viewing this topic.

Chameleon

great start everyone  :) I have some experiments to show its only been a year since the class and im finally getting round to having a go ...


ladies by Chameleons Photos, on Flickr

GlassBeadArt

Becky, these faces are AMAZING!!!
I am not terribly inspired for the moment, so I am mostly making spacers and small simple sets.
These are one of my favorite colour combinations: turquoise, purple and raku:

helenfc

Gorgeous faces Becky!

Here are some more dots, you are probably bored by now, but I was thrilled to pull these out of the kiln!


Medina by helenfchalmers, on Flickr


Damascus by helenfchalmers, on Flickr


Karelia by helenfchalmers, on Flickr

And a (very simplified) go at Mindy's B&B Tutorial!


Moogin style poppies by helenfchalmers, on Flickr

Sorry for the hog! (oink!) xxx

sundoorbeads

OMG Becky those faces are amazing :o
MadCat- TOTALLY loving all those beads :D
Here is Hilo new Organiks Focal
Keep Flaming! Michelle

Helen G

Lots of fab beads everyone, a quick post an run from me as heading out to the shedio to check yesterdays batch. 

Nothing terribly exciting but was rather pleased with this commissioned heart turned out  :)



And some sets of Pandora sized beads for an order.


Kaz

A commission!

IMG_0750 by Kaz ~ CheekyCherubDesigns, on Flickr

Just realised the dates on this gallery are wrong - Sunday is not 17th - it's the 13th! I'll go and change it!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Kaz

Sorry - can't resist posting these as well!
And then it's off to the shedio with me - to go dotty mad as I have just discovered a huge stash of the Reichenbach 96 intense transparent rods that you can use sparingly with 104 (like frit!)

Amber Pringles by Kaz ~ CheekyCherubDesigns, on Flickr
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

silverlemon

Wow. I thought I'd make notes on this weeks beads to post comments here.....I underestimated the size of paper I'd need...the beads here are phenominal.

Helen - Hels bels, they're fab
Becky the faces are so you
Helen lovely dots
Madeline I love the colour combo
Pris fab Clio beads
Les I love the first bead, and adore the look on the cats face in your banner
Sandy - just beautiful
Hil - nice shiney hearts
Swurlgurl, fab chocs, if only all chocs had zero cals
Kaz - nice dotty beads, love the etching
Helen, such precision flowers
Claire Louis - my jaw dropped when I saw your Rainbow organics
Manda - mangolo, stunning

I'm sure I missed some, was in a rush.

here's mine this week


Misty Sunrise by sarah downton, on Flickr

can't remember if Clio or Ehko


Lilac dotties 5 by sarah downton, on Flickr

Simple dotties


Montego Bay by sarah downton, on Flickr

Montego Bay
Bionic Sarah xxx    Sarah Downton On Facebook  My Etsy Shop

mummydude

Amazing beads on here (as usual!)  ;D

I think I got some mojo back after your suggestions and flicking through Passing the Flame  ;)


Ivory & Grey


Retro Dots


Vicki

mummydude

I managed to grab 20 mins in the shed as couldnt wait till monday!

I likey likey the shiny shiny!  ;D




Vicki

Lush!

Oh my my, I've only looked back a couple of pages and this is a fantastic Gallery.  I'm gonna post and run back to the beginning of the thread and have a proper look.

I'm working on some Seaside beads for an exhibition.  I dusted off my beadliner this morning and cored this one.


Seaside big hole bead by LushLampwork, on Flickr


www.lushlampwork.etsy.com

Princess Peggy (Priscilla McGirr)

I'm sorry ...I seem to be always posting my efforts this week, but I'm on a bit of a roll after a 2 month lack of mojo....

I'm always trying to do the impossible rather than stick to what I know, and this time it was see how long a bead I could make.  Very difficuly, as one end cracks before you finish the other, and then the middle cracks because you have been spending too much time on the ends!
However, I did manage six beads, most a bit mucky from re-melting parts of them, and two have small cracks...the longest is 82mm


Long beads by Princess Peggy1, on Flickr

And this is the one that survived as I planned it....75 mm long


Long bead by Princess Peggy1, on Flickr

Well, we're going to York for Valentines day, leaving tomorrow, so I can promise I definitely won't be posting any more pics for a bit.   
Pris
My Website http://www.dancingwithglass.co.uk  My Etsy http://www.etsy.com/shop/princesspeggy01
My Facebook page: https://www.facebook.com/DancingwithglassLampwork

Pat from Canvey

I made another goddess bead, this time in clear and put enamels on it.

MangoBeads

My new beads have become something of an obsession and our mandrels have come into their own. My new collection of beads are designed on random size mandrels from 6 - 12mm. They are designed to be worn on anything either stacked or the conventional threaded way. We will be offering chain and suede accessories for these. The beads are going to be sold as collections and some will be repeatable designs. None will be cored  ::)   and there will be plenty of them !!! ........ just had to share  
Sorry for the hog !  ::)

IMG_7840 by Mangobeads, on Flickr

IMG_7841 by Mangobeads, on Flickr

IMG_7828 by Mangobeads, on Flickr

IMG_7820 by Mangobeads, on Flickr

IMG_7823 by Mangobeads, on Flickr

IMG_7817 by Mangobeads, on Flickr

IMG_7842 by Mangobeads, on Flickr

IMG_7844 by Mangobeads, on Flickr
Sorry for the hog but thanks for looking  :)

Ilona

I have just a few piccies to show tonight, and will try to show some more tomorrow.