Hiya

As I've now been lampworking nearly 6 months, I have some idea of the glass I love.. and the glass I hate!  I'd be really interested in knowing your top picks in each category and it will be interesting to see if any themes emerge.  I work on a Hothead at present.

GLASS I LOVE (Well not all of it - that would be ridiculous, these are just highlights!):

Effetre Dark Lavender
Effetre Opal Yellow
Effetre Alexandrite
Effetre Dark Ivory
Effetre Red Purple
CIM Aubergine
CIM Sangre
CIM Elphaba
Effetre Coral
CIM Mink
Aurae
Triton
Luna
Psyche

GLASS I HATE:
Reichenbach Magic (it just stays beige for me)
TAG Dalai Lama and Tibet (ditto)
Raku (No good on a HH)
Double Helix Clio (contraversial, but I can't get anything but poop from it!)
Effetre Whisper (just don't get it)
Most Effetre Turqouises and Greens (go yucky on my HH)
Rubino Oro/Cranberry Pink (still trying to work it without it getting grey whispy bits in it)

What about you?


Sarah

Hmm Helen - I pondered what would be my five "can't live without" glasses over the weekend and came up with this:

Stoneground
Copper Green
Dark Ivory
Aurae (Light, Dark & normal)
Psyche
Red jasper
Seashell swirl
Clio
Psyche
Kronos
Sea foam
Rembrandt
Simply Berry
Hades
Aether

Seems I can't count.........

I've never been attracted to ghee and I don't get on with leaky pen

Sarah
xxx




sarah t

i have a love hate relationship with most of the glass i have depending on all kinds of things ...but have to say the hate bit is usually down to me  and my inability to control it ...not the glass itsself

there are a few i wont bother getting again ...annice white being one of them ....and i wont bother with filigrena rods or encased goldstone etc ...home made are much better!

Kaz

In no particular order...
Triton
Ekho
Dark Ivory
Kryptonite
Antique Clear
Dirty Martini
Multicolour Dark
Light and Dark Teal
Heffalump
Green tea
Vetro Key Lime

I dislike
Ghee
Petroleum green
Leaky Pen
and those funny CIMs like Olive and Adamantium

Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

helbels

Ooh exciting to see that there are 5 glasses already on your "love" list that I haven't encountered yet  ;D

helenfc

love:
Dark Ivory
Coral
Reichenbach Ocean
Dark Multicolour
Dark Silver Brown
Straw Yellow
Zachary
Mermaid
Dirty Martini
Elphaba
Freman
Stoneground
Hades
Red Copper Green

hate:
Effetre Striking Reds/Yellows
Laguna Blue (disappointing)
Effetre Clear
CIM colours that crack encasing

Havn't tried so many glasses though! Whats effetre alexandrite? and whisper? i like this thread :)

Trudi

ohh - I'm surprised that a few of you don't like Leaky Pen - tis a gorgeous colour!
What's Effetre Whisper - I've not come across this one!
My list I'll need to work on -

dislike -

TAG Jupiter - so much promise and it hates me. I haven't touched in months. Perhaps I need to give it another try ...... who knows amybe the magic will work?????????????
Magic  -but may give it another go when I'm in a rackless mood!
CIM Sapphire - beautiful colour, but a b*gg*r to work with!

Love
Tag Deep Purple - I've only just discovered this one!
Aurae - it rocks!
034 Turquoise
Pale Emerald
Pearl Beige - esp with ocean
Reicenback Opal Yellow!
Black Nebula - wow!
Gaia when it does what I want it to!
dark lavender
Bullseye Coral and sunset striker

This list can go on ........



helbels

Alexandrite is a lovely colour shifting greeny/purple and Effetre Whisper is clear with a pinky swirl in it - both I got from Frantz Art Glass in the USA.  Unfortunately my HH doesn't like the Whisper..

Josephine

Ivory
Transparent pale brown
Transparent baby blue
Transparent light emerald green
light turquoise
Triton
Aurae
Antique clear
heffalump
copper green
red roof tile
pink swirl
wasabi
pearl grey
mermaid

I don't like

pulsar...maybe i got a bad batch but it bubbles like mad
tongue pink
ghee
clear that misbehaves

helbels

Where do you get Black Nebula and TAG Deep Purple?  They sound ace!

helbels

My Pulsar bubbles too Josephine, but its such a stunning colour, I don't care!

SilverGems89

ok glass i love
Reichenbach Opal Raspberry (gorgeous pink that works on a hh with no problems!)
Reichenbach Flamingo
Effetre Dark Ivory
Effetre Copper Green
Effetre Red Purple
Effetre New Violet
Effetre Periwinkle and Dark Periwinkle
Effetre Straw Yellow
CiM Thai Orchid
CiM Heffalump
CiM Poison Apple
CiM Dirty Martini

and (very short list of) glass i hate
Reichenbach Iris Blue (just totally underwhelmed by it)
Effetre Rose (burnt a big hole in my carpet)
CiM Gelly's Sty (doesnt work well on my hh)
Effetre Silver Black (may just be me)
Reichenbach Multicolour (have yet to get anything but snot out of this)

So looking forward to trying some of the glass you have all mentioned so far!

helenfc

helen if you hate your effetre whisper do you want to swap a rod of it at flame off for something? i just got some vetro oddlots if there is a rod or two of them you would like to try?

helbels

Hi Helen

Yep, just let me check I've still got some - I'll send you a PM tomorrow if I have?  Can't check at this late hour. 

Helen x

Redhotsal

Love:

Eff Dark Ivory
Eff Rubino Oro
Eff Tequila sunrise orange (very old lot) and all of the other corals
Eff Turquoise
Eff Aqua
Eff Copper red
Eff EDP
Eff Opal Yellow
Eff Ink Blue
Eff Clear 006 - loving that glass

DH Terra - the king of glass
DH Psyche (though I can never spell it)
DH Triton
DH Aurae


Lauscha Clear - "Reassuringly" expensive

CIM Thai Orchid
CIM Ginger
CIM Leaky Pen

Reichenbach - Pink lady
Reichenbach - Iris Gold

Hate:

I have 2kg of Straw Yellow that I could cheerfully stand up against the wall and shoot.
Effetre so-called "cool" Strawberry Shake - which is a fancy way of saying plain dull white.
Some weird glass that can only be described as "sperm coloured". No idea what it is and what possessed me to buy it.
Effetre 004 "crystal" clear. Not.
Reichenbach - "Multicolour" - well as multicoloured as only green can be.
Reichenbach - "Magic" - as convincing as Paul Daniels.