Multicolour??!!

Started by Amber, February 28, 2010, 05:35:58 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Kaz

She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Yellow friend

After fiddling about with a lot of these new colours to get blues and purples etc., I wonder if I shouldn't just use a blue or a purple!
www.crocosmiajewellery.com
www.crocosmiajewellery.etsy.com

AnnaSpanna

I have failed monumentally to get any effect from this glass whatsoever on my HH so I took some home to pay on mum's minor and voila - my faith in this glass is restored. Just a shame I cant get get same effects on my HH!

helenfc

a couple of mine kiln struck to a deep wine red last night...i think its because i didnt encase them fully, whoops, but i quite like the effect. ::)

Krysia@No98

ooo I'd love to see a picture of that
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Amber

One of my encased ones is wine red and light yellow  ??? but it's in the kiln now, so we'll see what it looks like when it comes out! Oh, the suspense!  :D

madpup

Ok few from me using the multicolour,
and two marbles,
i used diffrent flames, white hot dripping off the mandel to a slow melt,
oxy flame, propane flame and in between, i found white hot oxy flame got the best colours for me.


Instead of getting married again, I'm going to find a woman I don't like and just give her a house.


www.madpup.co.uk

helenfc

mmm the marble on the left i really like! :)

Redkite

Ok, I can't resist any longer: off to Martin's website.....

kaatje

Quote from: Spookyjewel on March 31, 2010, 10:45:11 AM
One of my encased ones is wine red and light yellow  ??? but it's in the kiln now, so we'll see what it looks like when it comes out! Oh, the suspense!  :D
Are they out yet?
Love, Karin

Yellow friend

This Multicolour looks very similar to Pandora
www.crocosmiajewellery.com
www.crocosmiajewellery.etsy.com

Amber

QuoteAre they out yet?

Yes - and they've stayed the same colour!  :o An interesting glass this, I was finding it so easy to strike the MCD and yet the last couple of days I can't get it to do anything at all!  ??? Wonder if the waning moon has anything to do with it... :D

Trudi

Well I decided to have a go at encasing this glass - the dark one! I noticed as I started to put the clear on the colours went wild - but as I melted the glass in it went poo green. I did everything to try and re-strike this , to no avail. So I thought I might as well put them in the kiln - and boy - look what I found when the kiln faries had done their magic!


helbels

Pretty :)  When I encased the Multicolour Light and then annealed it,  I got lots of red bits that weren't there beforehand... which Reichenbach say is a reducing issue.. but it can't be as glass can't reduce once encased.

Trudi

Tis magic!!!

But I'm now wondering when using it un-encased if I should slightly understrike to see if it's striking more in the kiln!