Main Menu

gallery archive 09

Started by Sarah, December 29, 2008, 03:53:22 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Dee Dee

As I am in the future (?!?) and reach Monday before most of you, I thought I show you this hot one - Firestarter!





What have you been up to??

dinah46

What a lovely hot bead Steph :D

Here's how I spent yesterday afternoon, coring 27 beads :o



20 of them were made using Ekho on various bases and different patterns



I quite like the effect of them all together, I think I'm in love with Ekho ;D

Sarah

Emma your knobs are getting better and better! That heart is an absolute stunner  ;D

I have a few sets to show  :)


Sarah
xxx

Clare Scott

I`m loving your heart Emma - great work!
All those silver cores - wow!!

A few sets from me:

Amazon





Rose Gold




Dreams of Glass

Loving those sets Sarah, especially the top set, very bling   8) :)

Claire those are stunning, particularly the Amazon set.

A few from me, been burning the midnight oil again, daren't go in the cellar tonight, OH's forgetting what I look like, it's been 1am before I got to bed the last few evenings  ::)

My very favourite giant bat, a whopping 57mm.


A small red fairy with pink wings, little witch and yellow/orange fairy with yellow wings

and from the back  :)


:)
Ingrid                         
xx

Clare Scott

#425
Thankyou Saffie - hope you are feelig better soon.
Great beads as always Dora.

These are yesterdays offerings (If you are bored of my shard beads look away now!!)

Ethereal

(Remake of a set that is o the front page of Septembers Beads & Beyond mag thanks to Eve Smith ad her wonderful necklace!! Yay!)

Tyna

MyPrecious

Just thought I'd share my latest set with you!

(sorry for the bad photo quality, I haven't managed to find the right spot for photos in Paris yet)
Kathy

My website

turnedlight

They are, I'm so envious of her florals..
I have sold all my seashore beads so I made a few today, I used triton at tht top, and there are trails of 'multicolour' which are just bluey but nice, and terra bubble dots (ignoring the fuming behind the bubble dots, look how easy terra is to get purple, why oh why can't we have it back?!)

   

:)
kathryn

Tracy

I made a pair of earrings with some beads I made in my first month, nice and simple, I like em  :D


afina

Hi!
I made some plain beads yesterday.

Hope you like them!
Regards, Verena
Glasperlenwerk - My bead-site with blog (German) - http://www.glasperlenwerk.at
Vetromagic - Frit and fritblends in COE 104 - http://shop.vetromagic.at

sublimekate

This thread is awsome, really really beatiful beads.

I have another big beady picture, loved making these tabs, went mad with DH and Northstar and had a ball, bead making was fun this week, I love my job  ;D




Sorry Mods for super big piccy  ::) Kate xx

Ilona

Wow there are some amazing beads on this thread this week :)

Here are a couple from me




soulsilver

Just one from me this week. I have been longing after those gorgeous long tube beads that you see, so i finally plucked up some courage this week to give it a go!
Not all that long but a tube bead none the less.



Any advice from anyone on how to make those lovely long thin tubes? on a hothead?

bluefairy

Wow....brilliant work my lovelies!!  Fairly embarrassed to show this, but here goes.....
As some of you know, I got my torch in March, torched for about a fortnight then had, um, a bit of a blip, shall we say......anyway, started up again about 2 weeks ago, and these are the first ones I felt were ok enough to be allowed out in public  ;D



Sorry for rubbish photos, don't seem to be having much joy with them today  :-\

Have also got a couple of (VERY BASIC!!!) reactions, but guess I'd better put them in the challenge thread!!  ;D
Helen xx

My Etsy     My Facebook     My Folksy

Magpie

mmmm yummy bead posters Kate.

I got some time the last week or so to melt some glass....Fish, BHBs, and a focal pink with silver foil in that stayed pink!

Also 2 pairs of curtain pulls for my bedroom curtains.