Re: CiM "show and do tell" Competition

Started by sparrow, November 20, 2008, 08:05:09 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Magpie

Still more....

Eff dark ivory with chalcedony

not too bad

Magpie

And again

Eff dark ivory with electric avenue (or could be pulsar)

Nice, classic ivory/turquoise reaction.

Magpie

yet again....

Eff dark ivory with pulsar (or could be electric avenue, they both look transparent on top of the ivory)

and once again that ivory/turquoise reaction

Magpie

the last of the round ones.....

Eff dark ivory with french blue

my favorite

Magpie

the final one, I'll let you get some rest now...

The body is Eff dark ivory, mouth french blue, tail (from body outwards is halong bay, chalcedony, electric avenue and pulsar. There appears to be a reaction going on between the electric avenue and chalcedony


And that little lot are Donna's birthday pressie.  ;D

princess pink

another one from me, it's eff dark ivory, sis, and cim pulsar (the fourth one on the end)

had a lot of trouble with pitting and boiling with this glass so etched it which seemed to help smooth it over a bit


Trudi



These are Marshmallow and Kryptonite!
(Pandora stringer!)


Trudi


Trudi

Almost forgot



Kryptonite base with effetre roses!

T x

Trudi

My leaky pen misbehaves, must have a go super heating it!


Made on  a base of Chalcedony - with Electric Avenue & Ocean!

Trudi



Had a go at one of Les's cats - this is on pumpkin with magic!

Trudi



And a hollow crocus with fine raku frit!

Trudi



This is Pink chapagne with heliotrope frit!

Shadowdarner

#89
My turn! 

I used:
CIM: Celadon, Ghee, Creamsicle, Elphaba   Vetrofond: Light Topaz
Effretre: Biege transparent,  Dichroic strip, SIS (From Effretre Ivory) and a goldstone Effretre encased stringer



Don't ask me what it is though!  We're calling it a Stegosaurus bead! ;D