User contributions for Kevie192
Appearance
19 November 2008
- 12:2812:28, 19 November 2008 diff hist +22 N Hot head Hot head moved to Hot Head over redirect current
- 12:2812:28, 19 November 2008 diff hist 0 m Hot Head Hot head moved to Hot Head over redirect current
13 November 2008
- 22:2122:21, 13 November 2008 diff hist +4 Anneal Redirecting to Annealing current
- 22:2022:20, 13 November 2008 diff hist +19 N Anneal New page: #REDIRECT:Annealing
- 22:1922:19, 13 November 2008 diff hist +744 N Vermiculite New page: Vermiculite is a natural mineral. It expands when exposed to heat and is used frequently in lampworking. Many lampworkers use vermiculite if they batch anneal their beads. Used in... current
- 22:1022:10, 13 November 2008 diff hist +1 Frit Happens! →Where did the name come from?
12 November 2008
- 18:3218:32, 12 November 2008 diff hist 0 Hot Head No edit summary
- 18:3118:31, 12 November 2008 diff hist 0 N File:Hothead.jpg No edit summary current
- 18:2918:29, 12 November 2008 diff hist +28 Hot Head No edit summary
- 18:2818:28, 12 November 2008 diff hist +30 Hot Head No edit summary
- 18:2718:27, 12 November 2008 diff hist 0 N File:Hothead.gif No edit summary current
- 18:2618:26, 12 November 2008 diff hist −5 Hot Head No edit summary
- 18:2618:26, 12 November 2008 diff hist +810 N Hot Head New page: The 'Hot Head' is a lampworking torch which is used by many lampworkers when they first begin to make beads and is still used by many advanced lampworkers for some tasks. The main...
- 18:1618:16, 12 November 2008 diff hist +297 Lampworking No edit summary
- 18:1618:16, 12 November 2008 diff hist −399 Glass bead making Redirecting to Lampworking current
- 11:1611:16, 12 November 2008 diff hist +34 Sandpit No edit summary
- 11:1411:14, 12 November 2008 diff hist 0 N File:Charmbracelet.jpg No edit summary current
- 11:1411:14, 12 November 2008 diff hist +70 Sandpit No edit summary