trying to recreate a bead I like with soft white

Started by marijane, August 13, 2012, 04:00:00 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

marijane

I like the bead in the middle of the row near the bottom of this picture. I am reasonably sure I have got the right glass, soft white, a dark red and transparent black. The beads on the kebab have been annealed.  I've tried all manner of flame adjustments and stiking to get that rusty colour.  Any ideas?


523201_4354473941089_521498962_n by Beads by Mari, on Flickr

afina

Try a stringer of Ornela Ivory instead of the soft white (what colour and make is that?) - to me it looks just like that every time!
Regards, Verena
Glasperlenwerk - My bead-site with blog (German) - http://www.glasperlenwerk.at
Vetromagic - Frit and fritblends in COE 104 - http://shop.vetromagic.at

marijane

Quote from: afina on August 14, 2012, 08:42:17 AM
what colour and make is that?

It's Effetre 208.  I'll have a play with some other colours to see if I can get what I am after without the hit and miss element.   Thanks for your help.

afina

Ah, anice white! Is your red opaque or transparent? I get those reactions mostly with opaque reds.
Regards, Verena
Glasperlenwerk - My bead-site with blog (German) - http://www.glasperlenwerk.at
Vetromagic - Frit and fritblends in COE 104 - http://shop.vetromagic.at

Shirley

If you are looking for the rust colour to the red perhaps try turning your propane up a bit.
Val Cox Frit - Thai and Bali Silver 

marijane

I had another go today after referring to Kimberley Adams in The Complete Book of Glass Beadmaking.  She advised turning the propane up to melt in the stringers.  This made the line in the middle of the white wider and more grey looking.  I think it must be something to do with reducing / striking, I just have not found the right balance yet. Thanks for your help.