Main Menu

new reichenbach

Started by mindy23, September 02, 2007, 01:13:36 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

mindy23

Has anyone tried these new 104 colours yet that Martin has?  They look lovely but I was wondering if they needed any special annealing schedule?  It would be lovely if they went in on the ordinary Moretti programme but life is rarely that simple.  I have 2 different programmes on my kiln, the moretti and a Lauscha one that cools much slower, maybe that one would do.  I've been looking for a nice bright light orange for a while and this one looks perfect.

Love
Mindy



It could be much worse, but... it could also be much, much better...


Les

I haven't tried them myself.... but as far as I know.. if it's 104 coe, it *should* anneal like moretti..... unless anyone knows any different ?? If I remember, there were a few issues with CIM, or was it ASK ??

Sorry... I'm no help whatsoever... LOL... :P

Billie

There are several annealing schedules for CiM depending on the colour you use, which is painful and put me off trying the tester pack I got.    The new reichenbach will be interesting.  Martin should have an idea of the annealing schedule... or maybe it's worth doing a search on LE...?

Buzzybead

I've ordered them but I haven't yet got past the drooling over them and stroking them fondly stage. I was told to anneal them like Moretti.

Shirley

I saw them on the website yesterday. They look loooooovely! I don't need any glass but since when has that stopped me?  :D
Val Cox Frit - Thai and Bali Silver 

♥♥Tan♥♥

Need? nonono

want...yesyeysyesyesyesyes!!!!

*rowanberry*

Yeh it was the CIM with a different schedule - but that was only for 3  of their colours, cirrus, peacock and halong bay as they are the special "moonstone" glasses.

The other beads in the CIM range can be annealled alongside effetre etc I have found (though hadnt dora found difference?). Whatever, I've just been doing some testing for CIM and all except for the 3 I just mentioned were fine on my usual effetre cycle.
Claire

Maria Louisa

I didn't know this about the 3 CIM colours.
Can anyone PM me the annealingschedule for these please?
www.glassbeadsculptress.com
www.glassbeadsculptress.etsy.com
www.beadpress.nl
www.flickr.com/beadpress

*rowanberry*

I just do mine as I would effetre, but anneal at 550c instead.
Claire

mindy23

Hi everyone, thank you for your help. I've mailed Martin so I'll update here when I hear from him.  I never really NEED new glass but I always WANT it! 




It could be much worse, but... it could also be much, much better...


Maikki

I have been thinking this and when here is this thread I´ll ask loud: Do anyone knows if the reichenbach 104 iris glass acts like raku too?
Maija-Leena

*rowanberry*

ooooooooh a 104 raku!?! and its cheaper than terra ;-) please someone tell me its like the other raku :D
Claire

MangoBeads

I spoke to Martin today and its much easier just does its own thing easily ! Mines on the way !

*rowanberry*

my finger slipped and I just bought some  ::) bad claire....

too excited by 104 iris orange me, and iris blue! (I so loves iris blue...)
Claire

mindy23

Claire, when you say that you anneal the 3 cim colours at 550 can you put moretti in with them at that heat or do you just have to have a dedicated session using those 3 colours?



It could be much worse, but... it could also be much, much better...