lampworklover
yes, I managed to change my pic, only took 3 years
Forum Member
***
Posts: 238



WWW
« on: November 24, 2011, 09:14:02 AM »

I previously annealed some silver in my kiln, but only need to do a couple of small bits this time ....... is my Hothead hot enough to anneal silver?

(If not, DH's handheld kitchen blowtorch?)
Logged

Emerald
Forum Member
**
Posts: 80



« Reply #1 on: November 24, 2011, 10:18:10 AM »

The handheld torch will be enough to anneal if its not a huge piece, take it to a dull cherry red that should be fine.
« Last Edit: November 24, 2011, 11:57:26 AM by Emerald » Logged

lampworklover
yes, I managed to change my pic, only took 3 years
Forum Member
***
Posts: 238



WWW
« Reply #2 on: November 24, 2011, 11:26:04 AM »

The handheld torch will be enough to anneal if its not a huge piece, take it to a dull cherrybred that should be fine.

Brilliant, thank you!
Logged

Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.032 seconds with 18 queries.