I previously annealed some silver in my kiln, but only need to do a couple of small bits this time ....... is my Hothead hot enough to anneal silver?

(If not, DH's handheld kitchen blowtorch?)
Title: Re: Annealing silver
Post by: Emerald on November 24, 2011, 04:18:10 PM
The handheld torch will be enough to anneal if its not a huge piece, take it to a dull cherry red that should be fine.
Title: Re: Annealing silver
Post by: lampworklover on November 24, 2011, 05:26:04 PM
Quote from: Emerald on November 24, 2011, 04:18:10 PM
The handheld torch will be enough to anneal if its not a huge piece, take it to a dull cherrybred that should be fine.