Main Menu

Iris Frit

Started by Trudi, May 30, 2007, 01:51:42 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Trudi

Hi

I've just had a play with Iris Gold Frit and was blown away with the effects!! Can anyone tell me if all Iris Colours have similar effects or is the gold one a bit special?

Thanks

Trudi

♥♥Tan♥♥

Hi Trudi, ok I am no professional but I think all the iris colours do something but they do need striking or reducing. I think if you leave them raised as stringer or dot decoration and reduce they are metallic. If the frit is melted in I found it bleeds and fades outwards in a really nice way.

  Do you know how to make stringer from frit...its only heating and dipping a clear rod into it, melting the frit in and then pulling it into a stringer, it may be lumpy though so beware ;D

*rowanberry*

Iris blue.... on ivory, silvered ivory especially... it went all lovely and wierd and green and things.... Also iris black did some interested spreading out stuff on white once when i applied it as dots....
Claire

Mary

I've seen the faux boro done with iris blue and iris green.

♥♥Tan♥♥

You cant leave us hanging Mary.....tell us more :D

Mary

You know Tan, the Effetre light brown dipped in frit, with or without silver, and pulled into stringer. These were done with iris gold, encased. Anyway, I've seen it done with blue and green too, though I've not tried it.  I do love the magic of getting these colours from brown and gold!


mams

Ooo lovely Mary.
Thanks for the stringer tip Tan,I've learnt so much on here. :)

♥♥Tan♥♥

ah I bought some light brown to give that a try...hahaha thats in lots of bits now....but I shall salvge em!

Trudi

Cheers!!

I had a sample of Iris Gold and made somw faux boro beads  -and was amazed with the results - I also pulled a stringer and tried it on different bases!! I'll propaly have a go with differebt frits next!!

T

Phoenix*

Quote from: shine-on2 on May 31, 2007, 07:42:14 PM
Cheers!!

I had a sample of Iris Gold and made somw faux boro beads  -and was amazed with the results - I also pulled a stringer and tried it on different bases!! I'll propaly have a go with differebt frits next!!

T

show us then Trudi!!!!!
Kim :)    &  www.phoenixbeads.co.uk

Trudi

Sorry - I haven't posted pic yet - the shame!!

Here are a few that I've made:


The Iris Gold & Iris Green are great - someone sent me Iris Blue and I have losts of trouble with that and not very good results!

♥♥Tan♥♥

those are very yummy beads

*rowanberry*

oh they are lovely - did you do anything special to it, like mix it with the straw yellow/light trans brown? or is it just the frit?

As for iris blue - try it over silvered ivory...
Claire

♥♥Tan♥♥

haha is this tips from pointy tits ;D

Trudi

Oh - great tip about the iris blue - I'll give that a go!!!

For the ones in the picture nothing too special  - generally an opaque base  -  - then either a matching stinger with the frit only roughly melted in - about 3 times then pulled over the base and covered with a light transparent. I've been trying different combos to see the effects. and it's stunning! I just need to work on the encasing a bit more - but hey - it's all practise!

Cheers!

Trudi