Iris Gold Frit - 104 or not?

Started by Kimster, March 16, 2014, 03:56:35 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Kimster

Does anyone happen to know if Tuffers Iris Gold Frit is 104 or not? It doesn't say on the bag.... :-\

Shirley

Unlikely. You'll be fine using it anyway, unless you are planning a really thick layer. Most frit that is used with 104 glass is between 89 and 96 COE. I use it all the time and have never had a problem.
Val Cox Frit - Thai and Bali Silver 

Kimster

Thanks Shirley. Just encased a few anyway :)

tuffnell glass

Hi ,
   Iris Gold Frit is a Reichenbach glass frit and is 92coe . As explained earlier if only a surface decoration you will be fine .

Best wishes ,

martin

tuffnellglass@yahoo.co.uk
www.tuffnellglass.com
www.flameoff.co.uk

Kimster

Thanks Martin - they've all survived anyway  :)