Does anyone happen to know if Tuffers Iris Gold Frit is 104 or not? It doesn't say on the bag.... :-\
Unlikely. You'll be fine using it anyway, unless you are planning a really thick layer. Most frit that is used with 104 glass is between 89 and 96 COE. I use it all the time and have never had a problem.
Thanks Shirley. Just encased a few anyway :)
Hi ,
Iris Gold Frit is a Reichenbach glass frit and is 92coe . As explained earlier if only a surface decoration you will be fine .
Best wishes ,
martin
Thanks Martin - they've all survived anyway :)