Main Menu

gallery archive 13

Started by Pat from Canvey, December 31, 2012, 09:51:41 AM

Previous topic - Next topic

0 Members and 4 Guests are viewing this topic.

helbels

That bracelet is delicious, I love the purple tones in the beads, they are fab x

tish

ok i have a lot of beads to show all at once i make beads daily and save them up to go into the kiln


mel

My goodness, all stunning, a bit scarey to follow with my experimentals-although I was very pleased with my kelpy seaweed in the bottom one.


swirlylentil by melanie.ingledew, on Flickr


experimental by melanie.ingledew, on Flickr


seascape2 by melanie.ingledew, on Flickr


seascape1 by melanie.ingledew, on Flickr
Laughinglass Lampwork Beads

helbels

They are smashing Melanie - amazing for experimentals!!  Tish - what a lovely lot of beads, your kiln must be a biggun!

tish


GaysieMay

www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

CarolB

I'm loving them all especially the orange set it's my favourite colour :))

Kalorlo

Helen, I adore all three of those sets, but especially the marbley ones!
That bracelet is lovely, and the dark blue spacers really help it pop.
Tish: what a haul! I like the orange fritty ones and the dark purple pillows - they've got texture.
Melanie: ooh, seascape 2 has fab shapes and colours in it.

Here are the medium harps. The carnelian one at the top discoloured a bit on the harp side. I really like the ivory one. (This is why I try to stand lentils up to photograph them! But can't do that with this many  :P)


Dee Dee

WOW Amber, that is a stunning bead, no wonder it's a keeper - like looking into space!
I love your gremlins Heather, and the harp lentils are great!
Fab beads Sal, but adore your sculpture (I haven't got the bottle to have a go!) - and her boobs are so pert lol!
Love the sparkly set Helen!
That's a gorgeous bracelet Rita, and the clasp is divine!
Wow, loads of beads Tish!  I really like the yellow and purple combo, not one I'd have thought of!
Not surprised you are pleased Mel, the sea ones are particularly lovely!


Really spooky, but I was making the exact same beads as Helen's black and white stripy ones yesterday, but won't post them!  Instead here are a set of Inner Depth beads, I've got a beautiful batch of Multicolour Dark that you don't even have to try with - will cry when it's all gone!!


INNER DEPTH - Multicolor and Black Lampwork Bead Set by Beads by Stephanie, on Flickr


INNER DEPTH - Multicolor and Black Lampwork Bead Set by Beads by Stephanie, on Flickr


Shirley

Val Cox Frit - Thai and Bali Silver 

Dee Dee

Quote from: Shirley on March 25, 2013, 10:56:10 PM
What a sad face, Steph!

It is too!! I never noticed - maybe I should reshoot lol!

Alison G

Great as always ladies and gents. I have really lost my mojo lately but the excitement of FO and the thought of seeing Lucio again has given me a bit of a lift, plus I have a one to one lesson with Di East on Sunday so I'm hoping to be back at it.

Dee Dee I bought a tut for those style beads a while ago now but I've never got results anywhere near as brilliant as those, well done!
NB. Do not touch hot rods of glass, it is stupid.

Dee Dee

Thanks Alison!  I'm thinking of doing a little video of me making them, to help my customers, but need to work out how!!

helbels

Steph,  please post your  black and white beads!  Bet they will put mine to shame,  but I don't mind!