Kalorlo

I made a witch gremlin!



I started playing with some new-to-me silver glass. These are tests to find out what they do, so aren't decorated any further.



1. Precision Van Gogh: came out quite dark but also had a lot of shaping. I do like the swirly blues. Will have to see if I can get it to stay lighter or use it on a light base. Think it would make good landscapes.
2. TAG odd Light Tibet, reduced and encased. I like this, it's very ghostly and has inner light that's not easy to photograph.
3. Effetre silver #1 (transparent aqua rod), reduced and encased. This reduces really easily and also unreduces really easily. You can see a patch of extra-reduced bronze.  I like this a lot. It looks nothing like the paddles on Frantz, though, so I'm unsure whether it's the same stuff! (Number on the rod is 591718: the Effetre silvers got new numbers at Frantz when he got more after the initial samples).

This last one is Lauscha silver crystal - I have a little bit to test. Over Lauscha transparent red, reduced and encased. This glass turns out very yellow - on its own as a base you can't really see the blues and greens at all from most angles since they get overpowered by the yellow. I put it over red to get them to show up: they do, but the whole bead still has a yellow tint that doesn't work very well, I think.



I have a whole kiln-full to check out tonight :)

Kimster

#856
Just posted in last weeks gallery by mistake  :-\ ....try again! With correct size photo this time as well. It's the first time I've posted in the weekly gallery so bear with me! I bought Pricilla's brilliant 'Beginners silver glass' tutorial last week, & had a go yesterday - my first real attempt at a set. I was pleased to get some colour, though everything else went to pot.. (bead shape, spacings, dots etc etc) Thanks again to Pricilla for very kindly talking me through the problems I was having on a Sunday afternoon  :)


GaysieMay

Love the gremlins Heather and the skulls Jean.  Beautiful colours Kim, I can already see them made up into a bracelet in my minds eye.  Here is a bead I made with some of the glass I didn't turn into beads on Bronwen's class.  I have to wait til Thursday when I'm going to Tuffnells to get the rest boo hoo - so I made another last night - even though I was tired after work and working by candle light (well almost with my silly energy saving bulbs)


013 by GaysieMay, on Flickr

Not the best photo but to say I'm chuffed to bits with this little fella is a massive understatement!
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

Sin

Nice job everyone! Gay, what a fabulous bead! I like it very much!

And how does my preparation for autumn market look like?


helbels

I have some sparkly beads to show today.

These are very me (and I just know that Gemma will be along in a minute liking these!):


007 by Alchemy Lampwork, on Flickr

and then I have a nice bluey green set too:


009 by Alchemy Lampwork, on Flickr

Thanks for looking

flowerjasper

#860
lovely beads Sin and Helen they are just FAB!
Had a couple of hours this afternoon, so glad I decided to go in the shed with Jane Perala`s tut,
really enjoyed making these  ;D
will make more for BOC

sandy

Sin


009 by Alchemy Lampwork, on Flickr

I prefer this blue-green set, Helen, really love this colour! Yum!   

Kalorlo

#862
I'm a teal person too  ;D
Love the Jane Perala chickens!

This bead is for the Autumn challenge on Craft Pimp and uses twisties and shards from a couple of Mini Mos. It's one of those beads that had so many things go wrong while I was making it that I can't really tell I like it or not  :P (Smudged twisties, broken bead release, glass on mandrel...)



I love this one, though! For the reactive twistie and murrini challenge, it's got my Perihelion murrini on it. Everything's thinly encased. Yes, I think I might make more of those!



Now for the rest of my silver glass playing.



It's a quietish gallery, so you can have all the details!  :P
Everything's reduced and encased in 006. For glass that I knew was striking, I got it very hot on the rod before putting it on the mandrel, and then marvering it out to a cylinder was usually enough to strike it.



1. Unlabelled. Think it has to be Ekho or a similar test batch. The rod was amber with a visible core, which my ekho doesn't have, but silver glass may vary... It also has a wrap on each end on top of the black.
2. Precision Sasha's Silver. Base is pearl beige. Love it!
3. Precision Van Gogh. Very dark, not a good look.
4. TAG Blue Realm. Love this.
5. TAG Taxco. Like it, but the Blue Realm's better!
6. Effetre Silver #3. Lovely colours, tiny bit of iridescence.
7. Effetre Silver #4. Not so good when used like this. Has some iridescence but needs to be combined with something else, I think.
8. Precision odd Silver Seaweed over pearl beige. Had no idea what this one did, have since looked it up. It's a striker and I think it needed much more deliberate cooling than it got here to bring out lighter blues and greens. (I also used it to swirl my autumn lentil: it went lighter on the back though you can't see that so well from the photo).
9. Supernova. I thought I'd try it again based on what I learned from using blueberry, so this is supernova melted in a reducing flame, shaped in neutral and then reduced and encased. It did something! Quite nice at the ends, over-reduced in the middle. So those of you with it, try beating it up a bit more.

Princess Peggy (Priscilla McGirr)

Probably not going to sell this one as it is a sort of prototype, but I thought I'd show it.  Both sides of the same bead which is a 40mm lentil.


Bouquet by Princess Peggy1, on Flickr


Bouquet reverse by Princess Peggy1, on Flickr
Pris
My Website http://www.dancingwithglass.co.uk  My Etsy http://www.etsy.com/shop/princesspeggy01
My Facebook page: https://www.facebook.com/DancingwithglassLampwork

helenfc

Looking lovely this week everyone, Helen, the dichro ones are stunning! and Sandy's chooks, and everything :)

Here are some more bicones from me, graffiti and grunge :)


East Village Graffiti 3 by helenfchalmers, on Flickr


East Village Graffiti 2 by helenfchalmers, on Flickr

xxx

Les

I'm late in here this week, and there are just way too many beads to comment on them individually ... they are ALL beautiful .. you brilliant lot !
Here are a couple from me

A bead for my new set of synthetic dreads :)


IMG_0730 by Mad Cat Glass, on Flickr

and a set for Halloween :)


IMG_0727 by Mad Cat Glass, on Flickr

Hope you approve ? :)

les xx

Kalorlo

I did some more testing earlier this week.



Lauscha silver crystal reduced with various bases and encasements.



1. Encased in forest green. The crack originates on the other side from a lump in the bead release and only showed up when I took it off the mandrel, so I don't think the glass is to blame.

2. Over a base of 081 dark lavender, reduced and encased in more dark lavender. Dark lavender colour-shifts: looks pinker under incandescents.

3. Over transparent cobalt, reduced and encased in Effetre 006.

4. Over Effetre black, reduced and encased in Effetre 006.

spexy

The thing I love so much about making lampwork beads is the diversity. Here is some of what I made the other night.


Tourqouise and Coral focal bead by Earthshine Lampwork Bead and Jewellery Design, on Flickr

I made the poppies using enameled stringer and strangely they didn't etch. I like the effect.


Poppy Floral Bead by Earthshine Lampwork Bead and Jewellery Design, on Flickr

There is a challenge on Bead Buddies (Facebook) using Iris Orange and a transparent glass, this is my best attempt. Still can't manage to get any decent colour unless I use dots or frit.


Floral Lampwork Bead by Earthshine Lampwork Bead and Jewellery Design, on Flickr

This is Reichenbach transparent Silver Brown. Still having trouble getting anything consistant with it but I like these anyway.


Silver Brown ornate Beads by Earthshine Lampwork Bead and Jewellery Design, on Flickr


and I made this bracelet using one of Faiths lovely toggle clasps and I love this combination of hot pink and copper. A bit tricky to photograph.


Hot pink and copper bracelet by Earthshine Lampwork Bead and Jewellery Design, on Flickr

Kalorlo



More silver glass testing!

Sue sent me a bit of the BellaDonna, Garzoni Giovanna and coral lotus to try.



1. TAG coral lotus. Over black and on its own with a clear spiral.
2. BellaDonna purplescent. The dotty bead's a bit fugly and over-reduced (it has a core of half black, half clear, a purplescent spiral, encased and dots on top). The cylinder is over emerald green and has shiny oilslick colours.
3. BellaDonna moody blue (2 views of the same bead). Black cylinder, raised trails. The bit on the right of the bottom view where it's going greeny-ochre is over-reduced.
4. Precision Garzoni Giovanna - I do like this, but it's very similar to the golden emerald (when used like this, anyway!). Just a tad more opaque, which could be down to the amount of reduction.
5. TAG golden emerald
6. Precision black pearl spiral over clear. Really like.
7. Precision Rocio Silver Mist
8. Precision Abe's Ivy

Finally, a prototype gremlin skellington!


Trudi

They're great Heather!! You've really got some great reactions from all the colours!!

I've been playing with frits!


Delirious Glamour Rocks (1) by Glittering Prize - Trudi, on Flickr


Golden Peach Glamour (2) by Glittering Prize - Trudi, on Flickr

and these were one of the DH test batches over white!


Just Peachy by Glittering Prize - Trudi, on Flickr