Main Menu

gallery archive 12

Started by Madam Steph, January 01, 2012, 12:41:00 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

awrylemming

Nice to see your beads again Rachel  ;D  And I love the retro beads Sandy  :)
I have a couple of stripe sets.

SDC12278 by awrylemming, on Flickr

SDC12288 by awrylemming, on Flickr

helbels

Sandy, love those Retro Rogers, and stunning work as always Rachel.

Here are a few humble offerings


022 by Alchemy Lampwork, on Flickr


020 by Alchemy Lampwork, on Flickr


012 by Alchemy Lampwork, on Flickr

Madam Steph

First set using my new medallion press.

Gorgeous shards are by Jolene Wolfe and I have added some fine silver to some of the ovals:





Linda x

tomcat

tail end charlie here with a late entry to the week

well I had to play a bit more with this shape, think i will be doing more of these in different combinations



terra2 over adamantium - love the way it turns the adamantium chocolate brown

Mark - Blog - http://beadsbeerandphotos.blogspot.co.uk/
Life is not a game - its THE game, so play it like you mean it
A Long time ago in Egypt cats were worshipped as Gods, cats have not forgotten this !

GaysieMay

Up bright and early today, so guess I can start this week gallery?


ready for making up! by GaysieMay, on Flickr

I'm hoping by next week these will be bracelets!
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

mel

Love the sets Gay, especially the lefternmost ???  one
Etched blues are lovely too and the heart is intriguing.
I'm still on the trail of the watery theme.


clear seas by melanie.ingledew, on Flickr


blue oceans by melanie.ingledew, on Flickr
Laughinglass Lampwork Beads

MadelineBunyan

Gay, they are lovely, the first one is my favourite, the murrini work really nicely with the caribbean sea
Jeanie, that is totally not what I expected the seeded pink to be like, tis very unusual, works well with the frit colours.
the murrini on the etched turquoise is great, I like how they are all different like jellyfish 'swimming' about (is there a word for the way they move? I want to say skooshing but I think I made it up!) the ones in finding nemo are particularly coming to mind!
Mel, clear seas is beautiful, such soft colours. and I'm not usually one for pastels or pale transparents.

well...as I said, soft, delicate, pastel..its not really my thing...though I may sometimes like them, I dont make them!

so, here is something not at all pastel, or soft or indeed delicate really! they're not small, about 4 or 5 cm across.


Necklet Centre - purple and more by madelinebunyan, on Flickr


Necklet Centre - Flower side 1 by madelinebunyan, on Flickr

these are both now made into necklaces and will be off to a gallery shortly, but I loved making them so there will be more...and I have some other cool ideas for them which I'll reveal when they're done. oh and the bottom one has a curved hole.

Madam Steph

#367
Arghhhhhhh!!!!

Fancy having to follow Madeline's loveliness  :D

Here is a focal from me that started off as quite a different design, and my first set of this week:



The focal I call Hathersage and the set, Loxley.
Do you see a pattern emerging here?  :P

Linda x

soulsilver

Madeline those beads totally stand out for me, they are utterly stunning :)

A couple from me, some new Redhead Fairies, some tree spirits that came about after I had to remake 11 fairies that I accidentally smashed and a couple of Ellies, apologies if you have seen these already on FB or Flickr, and apologies for the hog :)

Redhead by soulsilver1, on Flickr

Red Head by soulsilver1, on Flickr

tree spirits by soulsilver1, on Flickr

Ellie by soulsilver1, on Flickr

Ellie by soulsilver1, on Flickr

spexy

So much loveliness already and it's only Monday!

I have been working on petal beads, the one on the right is my last and best so far. Now I need to practice on the consistancy of size.


Ciel

I've made quite a few sets last week, but this is a selection of them - I went a bit silver glass mad!





PeterG

Love the seeded heart.  I had forgotten I had some rods.  I'll see how they turn out tomorrow morning.

Here's some bubbles from me.  I rather liked the effect of the background through the glass.



Peter

LampyLou


First Fishy by Skarda Glass, on Flickr

I just wanted to share this little fella.  I wasn't intending to make a fish when I started but scales on a lentil bead have to end as fish..... apparently.  I think if I try another I'll have to look at a tutorial as his nether regions are a bit messy.

Julia x

MyPrecious

#373
Gorgeous work this week!

Gay - All beads are lovely but the first set is gorgeous!
Jean - Beautiful!
Mel - I truly love that first bead!
Madeline - I've already told you how much I like this bead!
Linda - Pretty colours!
Sally - Your beads are really cute but I love the colour in the pink fairy's dress.
Ciel - Gorgeous! Your petal beads especially. ;D But then again, I do love flowers...
Peter - Love the bubbles!
Julia - Cute fish! I love the scales. :)
Spexy - Truly gorgeous!

Here are beads I made last weekend:


Tropical Spring by Kathryn Greer, on Flickr


Last weekend's Creations by Kathryn Greer, on Flickr
Kathy

My website

Kalorlo

Kathy: love the egg-shaped ones.
Julia: Fishy!  ;D
Ciel: those are lovely!
Sally: hooray, more ellies!

I made some barrel beads that I'm going to make more of for a set. They've got a silver glass wigwag and the dots on the ends are Terra 2: comes out very different on each colour!



This is a pendant topper. You can't see so well here, but it has the same wigwag around the sides. Murrini by Kaz.