show and tell archive

Started by mummydude, July 15, 2010, 06:11:16 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Galloway Beads

#15
Some Hydrangea blue nuggets from me


IMG_3683 Down on the Beach by Galloway Beads, on Flickr

Elaine x

www.gallowaybeads.co.uk
My Etsy http://www.etsy.com/shop/Gallowaybeads

SueP

I must order more frit soon :)

Champagne Rain - love this frit



Bea's Bonnet



popped them in the Gallery as well so apologies if you have already seen them :)

Purplicious

I bought a couple of Bead Shapers from Bev last weekend in Manchester and promised her that I would post the first beads I made with them (sorry the photos aren't great, but there wasn't much daylight today!):



These are CiM Eggplant, Sherwood, Atlantis and Rainforest



These are CiM Dirty Martini with Val Cox frit Purple Rose - I'm really pleased with these, as they have a nice antiqued appearance.

Kathy

Isabelle

Did I mention how much I love my bead roller?? I'm saving up for more! ;D


Pandanimal

I am worried that people dismiss little beads. "just a spacer"  :'(

But I really love making them. So not surprising I have so many.
I worked out that it takes me roughly 5 minutes to make and clean each one. And that is when I make several on one mandrel.
I hate to think how much time my sorted box represents  :o


   

I also love the flexibility they give to a finished piece of jewellery when used en-mas in a bead weaving style.



This is my most costly etsy item so far. I wonder if it will sell? eek! But it was just too lovely not to offer up to customers.

Tiny beads. The possibilities are endless.


JKC

#20
Most of mine are gone to live with friends or unfinished.  Here are some of my uncompleted tiara small beads,  the model was very unhelpful.(not my lovely husband)


IMG_0819 by jntcasey, on Flickr
IMG_0817 by jntcasey, on Flickr
Unfinished tiara from scratch by jntcasey, on Flickr
replaced pearls with tiny beads by jntcasey, on Flickr

Sorry it's so big, it all went a bit wrong when I was posting.

MadelineBunyan

I've been putting this off for ages...

heres a few beads with my wig wags





more on my blog

so, where are yours? a number of you have got some of my wig wags now, so what have you been making?
or if you make your own wig wags, show those too!

Veebee

#22
OK, I had a good ole play at the weekend, what fun! I think I'd better do these as separate posts.... ::)
;D

This is First Love over clear and encased:




The bead on the right does indeed have an incompatibility crack. Why? Well, First Love contains Fuschia Pink, tricksy on a Hot Head. You can see that the cracked bead is darker, well I worked it a bit hot (lower reaches of the flame) and marvered it several times before encasing. As a result, the Fuschia reduced and this is what has caused the crack. I kept the left hand bead further out in the flame, melted it slower and only marvered it twice before encasing. Problem solved!
The paddle has some silver on it, Val doesn't reccommend silver with this blend as it can cause black lines around the pinks and oranges, but I tried it anyway in the name of scientific research.. It does cause black lines, but I didn't find it too bad.
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Veebee

#23
These are bea's Bonnet over Reichenbach Gold Ruby Bright and left as surface decoration:




The peach has a tendancy to blacken if over worked, so if on a HH melt it slowly in the outer reaches of the flame and don't mess it around too much!
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Veebee

This is Limerick over clear (that was wrapped in silver foil whch I burned off):



Limerick has green aventurine sparkliness that spreads out and just looks wonderful under encasement:

Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Veebee

This is Boro Bora, over clear (which has been wrapped in silver foil and burned off) then encased:



You can just see hints of the boro like effects this method can give you, here's some close ups:



Yes, the close ups are from the same beads above. I think if I had played a bit more before encasing I'd have had more wispy boroness!
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

MyPrecious

I like it too, but the photos don't do it justice :


Clear Heart by Kathryn Greer, on Flickr

Some of you might have seen these at the Flame Off. :)
Kathy

My website

JKC

More small ones from me, the larger ones are just to help shown the size.

IMG_0833 by jntcasey, on Flickr
IMG_0830 by jntcasey, on Flickr

Pandanimal

Those fruit pastilles are fantastic.

I am tempted to repost these now.


Made on a 1mm mandrell, the smallest I have that doesn't melt through in the flame.

Veebee

I think Rio Nights and me are going to be very happy together  ;D



Simply over clear and encased.
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/