woo hoo !! I've just managed to blow a bubble for shards......but!

Started by kathsd, May 14, 2011, 12:09:00 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

kathsd

I knew that glass blowing course was a good idea!
ok so I've managed to blow a small bubble about the size of a largish marble,  ;D felt really chuffed, then wasn't sure what to do with it! doh!
So, once it's on inflated on the mandrel what should i do then? put in kiln and anneal? dump in water to cause it to shatter (did this and got frit!!! ::) so not sure that's right)or put in vermiculite to cool then smash?
please help cus I want to go and do some more now!
thanks peeps
Kath

Pat from Canvey

Keep on blowing until its the size of a large grapefruit, let cool then break up inside a large bowl or tin to stop shards going everywhere

kathsd

thanks Pat , I'll do that and see what it turns out like! off to find a large bowl......
Kath