dinah46

Lovin all the pleats Steph and Diane :D

Here's some ribbed mermaid beads with a bit of copper and silver

Copper and silver necklace and earring set by dilunah, on Flickr
apologies if you've already seen it on flickr ::)

julieHB

Lovely, lovely beads and jewellery!!!

Haven't produced much, as my oxycon is not very well. Luckily Martin will have a look at it next week  :)
A few more cabs:

Murrini ring cabs by JulieHB, on Flickr

And my second try making a ring top that fits Sabine's bases:

ring top by JulieHB, on Flickr
Julie xx

                           My Webbie - My Flickr

Shirl

Thanks Julie, I might just have to treat myself to some :)

This is a BHB I made this week from Ambers tutorial. Hope you like it :)


Pat from Canvey

I recently bought the Michael Barley Baleen tutorial and here's a couple of my efforts.
and
second bead, and
Sorry about the reflection of the bay window. I didn't go upstairs to use the light cube.

cbeadies

Those beads are amazing Pat, they look so complex. And gorgeous BHB Shirl.

I have been having a go with Triton recently, made these after reading Manda's tutorial in the new Creative Lampwork book. (Thanks Manda!) They are a bit difficult to photograph as the black one in particular is very shiny!



Kaz

A couple from me - trying to get a peacock feather effect!

IMG_9612 by Kaz ~ CheekyCherubDesigns, on Flickr

IMG_9616 by Kaz ~ CheekyCherubDesigns, on Flickr
Think the multicolour dark (seond one) works better than the iris orange raku.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

MangoBeads

Oakey Dokey apologies if these have been seen elsewhere .....
Colour Wheels ...




IMG_7570 copy by Mangobeads, on Flickr


IMG_7564 copy by Mangobeads, on Flickr

Lush!

So lovely and bright and colourful, Manda!

I've been playing with my new long heart press from Beadpress


Long Spotty Hearts by LushLampwork, on Flickr

and my new CG beadrollers


Pure & Simple earrings by LushLampwork, on Flickr


Pure & Simple focals by LushLampwork, on Flickr


www.lushlampwork.etsy.com

Pat from Canvey

I made some more baleen beads. This one is made with stained glass, while the next 2 pictures are of the same bead made with 104 glass and The grid showing the last picture is where I put the bead in the kiln a little too early and it shows the imprint of the kiln shelf. The middle picture is of the edge of the bead so that it looks a different size from the face view.

Blue Kiln Beads


Pure & Simple earrings by LushLampwork, on Flickr

These earrings are so feminine, would look great with a crisp white shirt.  :)  Did you make the ear wires yourself Julie?
Yvette Goodridge
www.bluekilnbeads.blogspot.com
www.bluekilnbeads.etsy.com

Kalorlo

Wow Manda!

Here are the beads I made for the colour swap - I've been really busy trying to get my website ready so not a lot of beadmaking the last couple of weeks!

My trial beads: our colours were transparent dark turquoise, heffalump, ivory, coral and periwinkle.



Final prototype:


Beads I sent:


Krysia: I'm using 2mm mandrels unless I specifically need something else.

Fruddy

I've been making big hole beads again.... they are SOOOOO easy on Manda's 5mm mandrels!!







And here's a bracelet that I made, I used silvered ivory and encased Kalypso for the beads (love that glass!!)


ScarletLeonard

I had a desire to try something different.

I just made two hearts.

Heart Beads by Scarlet Leonard, on Flickr

Happy moment.


dinah46

Love that pendant Mindy  :D

I've finally got around to coring a few beads, it's just too cold to go outside to make new beads.

Cosmos by dilunah, on Flickr


Swirling Pools by dilunah, on Flickr

sublimekate

Gorgeous work everyone, awsome colour combo's Manda  :o

Not been around much lately, thought I'd show my face, or rather my recent beads  :D

Been playing with Clio.......



Lightly etched these, must admit had my heart in my mouth doing it, I'm not sure the pics really show the effect but the beads have a nice soft dreamy glow  :)