Emma @ Tuffnell Glass

Hello It's me ;D I'm back!
Yes there was a mistake. We didn't spot it until the new batch of Stripped pink came in. The problem was that the first time we ordered it we thought it hadn't been sent as we had also ordered EDP. We had no idea what the rods would look like LOL and it turns out they had not sent edp just the stripped pink......er this is making no sense is it???
Anyway yes if it has the transparent core you have Stripped pink. It is a lot more expensive than the EDP so I guess in a round about sort of you you got a bargain  ;)
As ever, If you would like me to swop it let me know in a PM.

Em xx

helenfc

ha ha now you tell me emma, I've only got one rod left! ;)
best hold on to the expensive stuff and order some actual edp  :D

Kalorlo

Helen, when you've used yours, what colour has it been?

helenfc

sorta like i would have expected edp...used it on opal yellow with silver foil and it was a lovely shiny deep opaque purple...it definitely has a core just like the one in your pic though!

rocky

Oh, my EDP has a trans centre too, and I had some dots go translucent the other day. I thought it was odd ... so its striped pink! ::)
Deanne x

★★Terri★★

I got some EDP from Off Mandrel a couple of weeks ago - it looks just like the rods in the photo.  Not used it yet - never used it before.....gulp!!!