Sarah

Quote from: Trudi on April 07, 2010, 09:23:12 AM
Quote from: Sarah on April 06, 2010, 11:33:58 PM
I can't believe I missed out Terra nova 2  - I love the stuff!

Trudi - leaky pen just bubbles on me as does pulsar so that can be added to my hate list too!

Sarah
xxx

Sarah

When I first tried Leaky Pen it pitted like mad - I left it for a few months then tried it again (same rod) and it behaved!!! Go figure! Perhaps it was weather conditions, flame settings - not sure. But give it another go just to see - you never know! Colette had the same issue too!

Perhaps it matures like wine? I'll give it a go again over the weekend - it looks like it should be a pretty colour  :)

Sarah
xxx

soulsilver

If any of you want rid of your TAG jelly opal can you PM me?? :)

Redhotsal

Quote from: helbels on April 07, 2010, 06:46:23 PM
  I wonder if the TAG Jelly Opal is Sal's "sperm coloured glass" - sounds like it could be!
Um no. The suspect glass is very old - it may not even be glass.... :o

Kaz

What, you mean it may actually be........  :o :o :o Like petrified ??? (Like Fordite ???) OMG did someone get very excited by the glass ???
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Redhotsal

Heh - Fordite! Issat the same as Dagenham Agate?  ;D
No, not excited by the glass(!) (eurgh). In my experience - it's mostly women that get excited by all those, um, rods of glass. Men seem to prefer marbles.....
I did wonder that the glass might be an extremely long bundles of glue sticks for a while, but it's probably something quite prosaic as Effetre. Might be P+T. 'Orrible glass whatever it is.

Trudi

Omg I need to close my eyes!!!!

This thread really has been an eye opener!! Lots of good hints and tips with dome smut for good measure!!!

Redhotsal

Dome Smut?? Don't know where your twisted mind is heading here, Trudes. I only use mine for marble making!  ;) ;) ;)
Hehe! That's it - I'm off to bed.  ;D

sea-thistle

I also like cranberry
rubino oro
green tea

I agree Effetre 004 is the pits!

Trudi

Quote from: Redhotsal on April 08, 2010, 12:07:13 AM
Dome Smut?? Don't know where your twisted mind is heading here, Trudes. I only use mine for marble making!  ;) ;) ;)
Hehe! That's it - I'm off to bed.  ;D

It was late Sal and I was on the I touch - what can I say - you're leading me astray!

jammie

New name for  a glass then ....
dome smut! described as fordite like prosaic petrified sperm coloured glass.....would folks get excited over this one   ???

MyPrecious

I absolutly LOVE :

(depending on how I want to encase)
- Vetrofond clear
- Lauscha clear

- Effetre Rubino
- CiM Cranberry
- CiM Thai Orchid
- CiM Celadon
- Effetre Pea Green
- Effetre Sky Blue
- Effetre White
- Vetrofond Black
- CiM Ghee
- Vetrofond Tangerine Sparkle
- Vetrofond Pineapple Sparkle
- Vetrofond Transparent Grass Green

and pretty much any other compatible colours...

I hate :

All colours that "pop"and "spit" bits of molten glass in my face all the time... such as Effetre Anice White or Vetrofond Marbled Avocado
Kathy

My website

Krysia@No98


urm...

LOVE
Poison apple - Glass of the moment
All the mystics apart from red
The grass greens
trans cobalt blue
silver brown
Cool kiwi
Deep Purple Red
Pastel Yellow

HATE
Canyon De Chelly

Not overly enamoured with
Magic  (I did get multicolour to do something, but not in a bead)
Silver Black (I get better silvery effects from effetre black, don't ask me how!?!)


I really love garnet red, but for the life of me I can't get it to work for me, I just burn it.
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Mand

Quote from: Redhotsal on April 07, 2010, 10:57:45 PM
Quote from: helbels on April 07, 2010, 06:46:23 PM
 I wonder if the TAG Jelly Opal is Sal's "sperm coloured glass" - sounds like it could be!
Um no. The suspect glass is very old - it may not even be glass.... :o
Quote from: Redhotsal on April 07, 2010, 11:14:48 PM
. Men seem to prefer marbles.....

LMAO!

Glass - I love it all - except TAG Tibet which turned out like very expensive poo on a stick. ::) :P

AnnaSpanna

I love too much to actually list it all; but of particular note are:

CIM Peacock
CIM Gunmetal
CIm Ginger
Eff Periwinkle
Reich Ocean
Aurae
Triton

I hate:

Magic
Magic
Magic
Magic
Magic

Kaz

Quote from: Krysia on April 09, 2010, 11:08:01 AM
Magic  (I did get multicolour to do something, but not in a bead)
Very, very curious......
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!