Double Helix for HH or Kiln?

Started by helenfc, March 25, 2010, 07:48:01 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

helenfc

OK, since I cant wait any longer I'm compiling my shopping list for flame off. I promised myself a 1/4 of double helix (cant get too much as would rather save up for big girls torch...) and I was wondering which double helix is HH friendly? liked Aurae, have tried a couple of rods but nothing amazing...or would i be best to go for a kiln striker like pandora or nyx? any thoughts very much appreciated :) thanks x

julieHB

Triton, as well as Aurae, is very easy to reduce, and work beautifully on a HH.
Julie xx

                           My Webbie - My Flickr

Shirley

Psyche gave me best results when I used a hothead. Triton should be ok too.
Val Cox Frit - Thai and Bali Silver 

Veebee

Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

SilverGems89

i bought a mixed 1/4, although i got to pick mine out myself  :-\

helenfc

Quote from: SilverGems89 on March 25, 2010, 07:53:13 PM
i bought a mixed 1/4, although i got to pick mine out myself  :-\

have you tried any? im pretty tempted by triton, thanks guys :)

SilverGems89

Quote from: helenfc on March 25, 2010, 08:05:58 PM
Quote from: SilverGems89 on March 25, 2010, 07:53:13 PM
i bought a mixed 1/4, although i got to pick mine out myself  :-\

have you tried any? im pretty tempted by triton, thanks guys :)

Nope  ;D im too much of a wimp, and i cant figure out how to cover the holes without burning my hands off!

Veebee

Took me a while to risk that too, but it's worth it in the end!
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

helbels

I'm a Hothead user and thoroughly recommend Triton, Aurae, Ekho and Psyche :)  Can't really go wrong with any of them although Ekho's a bit trickier than the others :)

Kalorlo

Tinfoil! Get a long piece (I folded mine in half lengthwise so it's thicker), wrap it round and use the tails as a handle to pull it up and down over the holes. You can fold the edges over a little too after wrapping so it all stays together better.

Nikki

I love TAG Taxco from off-mandrel, works really well on the HH

Pip

I've heard that some people just use an oven mitt to cover holes but I use a piece of A4 paper folded lengthways 4 times and kitchen foil folded around it. The paper insulates a bit from the heat and because of the foil, it stays in the shape of your HH for easy use  :)

SilverGems89

right just been and got my list stash to let you know what i have
kronos 2, ekho, aurae, triton, psyche and terranova 2
im gonna have to have a bash at using them....eventually  ;D

Veebee

Quote from: Pip on March 25, 2010, 08:19:25 PM
I've heard that some people just use an oven mitt to cover holes but I use a piece of A4 paper folded lengthways 4 times and kitchen foil folded around it. The paper insulates a bit from the heat and because of the foil, it stays in the shape of your HH for easy use  :)

Ha! Paper? I haven't ever used paper in the middle, I'll try that next time, thanks!
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

helenfc

yep i used the tin foil for reducing aurae, simples! how about you try them tomorrow gemma and let me know?!  :P ;D