Main Menu

Rust Coloured Glass

Started by helenfc, February 27, 2010, 10:36:21 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

helenfc

cool, im still on a hothead, so no chance of an oxygen rich flame yet sadly :(
is the the same thing EPD does then?
thanks for that, goodluck with the exploding opals too!

llewennog

Its not always an oxy rich flame that can cause devit, sometimes you can overreduce using propane and get the same effect, Ive never used a Hothead :D  Opal had contracted and has broken. I need to cut them smaller from reading a thread on another forum.
Ahh well they are only $1 each :D nothin like experimental flameworking!