Trouble with Straw Yellow?

Started by Redhotsal, February 15, 2010, 06:26:00 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Redhotsal

I've just bought a shed load of Staw Yellow for Faux Boro but it doesn't seem to be working at all. It turns everything a really dark brown and is frankly poo.

Is this just me or is this happening to you too? Poor batch do you think??

Cheers
Sal

Kaz

They probably sold all the good stuff as a result of your DVD and yours was the old bit that was at the back of the cupboard!!
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Helen G

I bought some after the course with you and Di and although it does work a bit, I can't get it anywhere near as nice as the beads I made on the course, I thought it was because I didn't have you watching over me Sal  :-\

Katiequiggle

Oh thats a shame Sal.  I hate this variation in quality of glass.  I've got a batch of Rubino Ora which is complete poo, looks almost a russet colour and is horrible.

Shirley

Quote from: Katiequiggle on February 15, 2010, 09:51:27 PM
Oh thats a shame Sal.  I hate this variation in quality of glass.  I've got a batch of Rubino Ora which is complete poo, looks almost a russet colour and is horrible.

I had some of this and it still struck to raspberry in the kiln. Might be worth another try
Val Cox Frit - Thai and Bali Silver 

hollergrafik

my straw yello looks like light trans brown, I double checked but its deffo a slightly different colour and doesnt do the nice purples for me.

sea-thistle

Glad I didn't buy any straw yellow then, !! After buying and watching Sally's DVD.!! A friend gave me two sticks of  the straw yellow she had and we had a play with it ours  seemed ok. ;D

Jeanniegems

Thank goodness
I thought I was a numpty. I bought some like Helen after the course with you. Mine comes out browny green, nothing like yours Sal. I can breath easy then and wait for the good stuff to come through
Jeannie
www.jeanniegems.co.uk
www.jeanniegems.etsy.com

helenfc

I got some about a month ago now, and i cant get it to do anything lovely and faux boro-y, looks like pale trans brown? maybe i just havent got the hang of it yet though, not sure? :'(

Redhotsal

Hmmm.......okay, all those with a problem - did you get from Tuffnells or somewhere else?
I wonder what the procedure is - I've never returned a batch of dodgy glass ever but since I bought half a kilo of the wretched stuff and it isn't doing what it ought I'm thinking of returning it or something. I didn't want to do this as I thought it was just me but I'm not happy with it. :-\

julieHB

Sal, you have worked so much with straw yellow and the faux boro effect, so you definitely know what you are talking about!!
Julie xx

                           My Webbie - My Flickr

Jeanniegems

Yes Sal mine came from Tuffnels but it was last August/September. What to do ! I bought half a kilo too!
Jeannie
www.jeanniegems.co.uk
www.jeanniegems.etsy.com

hollergrafik

I got mine a couple of months ago from Tuffnells

Mand

Quote from: hollergrafik on February 15, 2010, 10:24:36 PM
my straw yello looks like light trans brown, I double checked but its deffo a slightly different colour and doesnt do the nice purples for me.

Same here and I thought it was just me being rubbish again! I think mine came from Martin too.

Dragonfire Glass

are you sure its not just wrongly labelled?
the colours are very close