I got some pink Ask  from Martin.  On his web piccie the main rod is light but the heated end is a deep solid pink.... how do I make that happen... I just have a lovely pale pink

Dragonfire Glass

the pink I got from Martin goes through a cycle of colour I think from pink to a purple to a blue.
the same rod shocks extremely easily so start off on the other side of the room and introduce it to the flame so slowly you may fall asleep!  ;D
my workbench is littered with chunks of the stuff & I'm trying to think of an effective way of using it!  :)

Colette x

Caroline

Quote from: littlegiggles on February 23, 2007, 05:58:07 PM
I got some pink Ask  from Martin.  On his web piccie the main rod is light but the heated end is a deep solid pink.... how do I make that happen... I just have a lovely pale pink

dunno Julie, never used the ask pink, is it a reducing colour?

Mary

I've read it's a striker - strike it in a neutral flame like you would transparent red.

littlegiggles

hmmm.... thought I'd tried striking...  could someone give me an idiots guide... what I do is let the bead cool then flash it through the top of the flame... is that right?

and it's not shocked at all....

Mary

You might need to do more than flash through the flame, gently roll it warm in the tip of the flame, but basically you're right. Cooling first is the important bit. I've not used the Ask pinks, I'm only guessing that might work, I'm afraid!

littlegiggles

Thank you ...  will try later tonight

Shirley

Colette, can you mash the bits up to make some frit?
Val Cox Frit - Thai and Bali Silver 

One Key Beads

As I understand it, passionate pink and ladies slipper are striking colours.  If you try www.arrowsprings.com/html/ask_104_colors.html
you will get a list of the colours and their characteristics, as well as some tips on striking and reducing the colours.

Hope it helps


Jeanette

Dragonfire Glass

mashing may be a good idea Shirley.
looks like I need to do a bit more research on its properties too.

Shirley

Must say, I like experimenting to find out the properties and effects I can get, but it could get a bit expensive sometimes!  :D
Val Cox Frit - Thai and Bali Silver 

bubblebabeuk

I have some of this, fab stuff! It is a striking colour, you have to really let it cool almost till you think its gonna break then reheat till REALLY hot then let the glow go and quickly dump in kiln! Viola! The key things is the cooling before the strike it self when the glass goes back to HOT!
HTH

glassworks

the ASK people have given out a brilliant pdf with info on the back about how to get the best results from each colour, and stunning colour pr0n on the front to see what you're aiming for - please email me if you want a copy as i cannot figure out how to link it here?..

cheers

Q

orodrago

I havent acquired the ASK pinks yet, but thought Id toss this out re: the shocky-ness of the rods -
With Anise White - famous for being shocky, I anneal my rods with a batch of beads, before using
the Anise - it doesnt completely stop the problem, but does reduce the number of explosions....perhaps its worth a go
with this pink?  (Which is on the wish list for next order!  :) )

glassworks

i've been playing with some of the ASK glass overnight - and i must say it is less shocky than i though it might be - i also found it very soft - it works really easily and doesn't burn off quite so quickly as some of the effetre yellows and dark blues for instance..

they all seem to strike and reduce pretty much as per the pdf... but they are stunning colours - WOW!!!.... we have a visit booked to kuegler as they make other glass too - slightly harder - but very highly rated in Germany...