Re: CiM "show and do tell" Competition

Started by sparrow, November 20, 2008, 08:05:09 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Pandanimal



Gelly's Sty egg with Rasberry sorbet frit

Pandanimal


Pandanimal



Cirus with victorian splendour frit swirled round it

Pandanimal



Clockwork orange. The large bead has pumpkin dots and seems to have struck to a deeper colour. I guess because it was worked more?

Pandanimal


Pandanimal



Khaki and triton.
The Khaki seems to react much more than the canyon de chelly to the dh glass.

Thats my hog over for the moment!

I have learnt a lot about taking photos and posting them doing this.
lots of fun! thanks.
I hope you all enjoy the results. I know I still have a lot to learn.

Julia

Pandanimal



I thought you might all like to see this one as well.
Its lipstick with a twistie of lipstick and stoneground melted in. Then I shaped it in my brass doming block and the stoneground bit went all rainbow colours. I have tried several photos of this one and this is the best I could get that shows the rainbow effect.
Very pretty. Is this raku? I have never managed to do raku before.
This bead hasn't been annealed yet so I don't know if it will change in the kiln.
Also, you can just see in the picture how the lipstick in the twistie is more brown than in the base colour of the bead, a reaction with the stoneground I guess.
Worth playing with this combination a bit more I think!

Good luck everyone in the competition.

Julia

Ness

chalcedony -  a lone bead.  I'm still practising my rounds!




I think I managed to keep the colour this time, sometimes it's gone a bit milky

Ness

Ingrid, I love your little 'cauldron' bead!  That's so cool!

More chalcedony - pillows, this time.  A girl can only practise so many rounds....



The small bead on the right went a bit milky - did I overheat it?

Ness

Last one from me: kryptonite, effetre dk ivory and SIS.


faystuart

Well here goes.... hope I've got this right otherwise you'll be looking at absolutely nothing!



fingers crossed!  ;)

Fay

faystuart

Here's another one



Hopefully this will have details of the glass I used

faystuart

I might just get it right this time..



CiM: Marshmallow/Crocus and beady sam frit

faystuart

YAY!!!!!!



CiM: Heffalump/Count von Count and Beady Sam Frit

Easy Peasy

Fay x

faystuart

She's on a roll



CiM: Hades
Effetre: Dark Ivory and SIS
Wrapped with fine silver