flowerjasper



Sarah

those are lovely reactions with black nebula

These are both painted desert from the same rod in the same session - the upright is super heated and it looks like the red has gathered at the edges. I wasn't expecting that!



Sarah

Well Sue it looks like egg sucking works  :) Such a shame about the crack  :'(

I have some spotty beads with vetrofond odd cotton & Nero Intense Black. There is a tiny bit of bleeding in the flat black spots but not much



Sarah
xxx


sparrow

Okay, finally got round to taking more pictures (but not to cleaning the beads beforehand - sorry!)

Sooooo:

Vetro Odd Lot light red jasper with CiM Thai Orchid - the more you heat it, the more it gets eaten (compare left & right)



Vetrofond Special red purple (VS291438) with copper green and effetre dark ivory, not heated too much



A bit more obscure:

Vetrofond Oddlot 917 Antique Amber Transparent with effetre dark ivory, effetre dark trans topaz, and 're-constituted terra' (not terranova, but the batch where they tried to remake the old terra) and silver wire



And Vetrofond Oddlot 917 Antique Amber Transparent with 'new terra' and silver wire on its own - the amber didn't like the wire  and made big puddles around it that looked like quicksilver or lead (sorry about the crap photo) :(

Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

afina

Hi!
I have three Oddlot beads here:

From left to right: Belgian Lace with Raku powder, Red Jasper, Marbled Avocado (with just a touch of Terra).
Verena
Regards, Verena
Glasperlenwerk - My bead-site with blog (German) - http://www.glasperlenwerk.at
Vetromagic - Frit and fritblends in COE 104 - http://shop.vetromagic.at