User contributions
From Fritipedia
Jump to navigationJump to search- 10:59, 4 March 2010 diff hist +27 Bracelet systems current
- 08:33, 5 January 2010 diff hist +114 N Devitification New page: Take a look at the link below to find out more about devitrification http://en.wikipedia.org/wiki/Devitrification
- 15:48, 11 February 2009 diff hist +2 Bullseye →Further information current
- 15:48, 11 February 2009 diff hist +77 Bullseye →Further information
- 06:37, 28 January 2009 diff hist +343 N Silver core New page: This is the process of placing silver cores throught the hole in a bead. This can be done in a variety of ways: Gluing silver rivets into the bead Using a bead press and silver tube Usi...
- 06:32, 28 January 2009 diff hist +3 Health and safety current
- 06:32, 28 January 2009 diff hist +334 N Health and safety New page: This is a very big issue within glass beadmaking and working with glass generally. There is currently little agreement about what should be included in Health and Safety information but th...
- 06:27, 28 January 2009 diff hist +119 Didymium current
- 06:26, 28 January 2009 diff hist +154 N Didymium New page: Visit this link for more information on appropriate eye protection http://mikeaurelius.wordpress.com/2007/12/25/visible-light-hazards-and-the-glassworker/
- 06:25, 28 January 2009 diff hist -1 Eye protection →Eye protection current
- 06:25, 28 January 2009 diff hist +127 Eye protection →Eye protection
- 13:50, 3 December 2008 diff hist +314 N Adobe Photoshop New page: Photoshop is software for your computer that allows you to "tweak" your photographs. Adobe photoshop can be purchased through many computer shops or on the Internet but if you just want a ...
- 13:47, 3 December 2008 diff hist +4 Photography
- 13:51, 20 November 2008 diff hist +760 N Stringer New page: Getting detail onto glass beads can often involve the use of stringer. Stringer can be made by the artist or bought commercially. Stringer can be used to get lines and dots on beads as wel...
- 13:46, 20 November 2008 diff hist +398 N Batch anneal New page: There are 2 main ways of annealing your work in glass beadmaking: you can either work to the kiln or you can batch anneal. Batch annealing is where you make your beads, cool them in [[verm...
- 04:52, 15 November 2008 diff hist +236 N CiM New page: CIM stands for Creation Is Messy. They are suppliers of glass which hs a CoE of 104 and is compatible with Effetre, Vetrofond, Lausha and the other 104 glasses. Visit their website for m...
- 04:49, 15 November 2008 diff hist +852 N Ventilation New page: When glass is melted to form beads and other shapes various gases and fumes are released. Using other things in lampworking to embellish your work can also lead to fumes, gases and dust. A...
- 04:43, 15 November 2008 diff hist +110 N Soft glass New page: ==What is soft glass?== Soft glass is glass that has a relatively low softening point, for example Effetre
- 04:40, 15 November 2008 diff hist +47 N Borosilicate New page: http://en.wikipedia.org/wiki/Borosilicate_glass
- 14:46, 14 November 2008 diff hist +170 N Gather New page: This is the term given to the molten blob of glass on the end of the rod. This is the bit of glass that you lay down onto the mandrel or you use to pull stringer.
- 14:44, 14 November 2008 diff hist +427 N Incompatible New page: Different glasses have different CoE e.g. Bullseye and Effetre. When these glasses are heated up and then allowed to cool the outside of the glass cools quicker than the inside... current
- 14:40, 14 November 2008 diff hist +15 N Mandrels New page: See mandrel