Reichenbach produce a limited range of colours in [[CoE]] 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the [[opaque]] Reichenbach 104 [[glass]]es on a base bead of a very soft [[opaque]] colour (for example [[Effetre]] White) have a "bleed" effect rather than a crisp edge when melted down. | |||
Reichenbach also produce a range of [[CoE]]92 glass rods and [[frit]]s, many of which are either [[reactive]] or [[reducing]] colours. | |||
==Reichenbach colours and stock numbers== | |||
=== Transparent === | |||
{| class="wikitable sortable" width=90% | |||
|- | |||
! width=50px|Stock Number | |||
! Colour | |||
! Properties | |||
! Reactions | |||
|- | |||
|L1011 | |||
|Crystal | |||
|clear | |||
| | |||
|- | |||
|L1012 | |||
|Crystal soft | |||
|soft clear | |||
| | |||
|- | |||
|L2011 | |||
|Violet reddish | |||
| | |||
| | |||
|- | |||
|L2012 | |||
|Gold violet | |||
|more violet than rubino | |||
| | |||
|- | |||
|L2013 | |||
|Gold ruby light | |||
| | |||
| | |||
|- | |||
|L2015 | |||
|Pink lady | |||
| | |||
| | |||
|- | |||
|L4015 | |||
|Antique | |||
|aka antique clear, is greenish | |||
| | |||
|- | |||
|L5010 | |||
|Silver brown | |||
| | |||
|silver reduction glass | |||
|- | |||
|L6015 | |||
|Garnet red | |||
| | |||
| | |||
|- | |||
|L6027 | |||
|Rosalin | |||
| | |||
| | |||
|- | |||
|L7003 | |||
|Amber | |||
| | |||
| | |||
|- | |||
|L9202 | |||
|Black | |||
| | |||
| | |||
|- | |||
|L5011 | |||
|Dark silver brown | |||
| | |||
|silver reduction glass | |||
|- | |||
|L9203 | |||
|Deep black | |||
| | |||
|may reduce metallic | |||
|- | |||
|L1012B | |||
|Ocean | |||
|blue with sparkles | |||
| | |||
|- | |||
|L1012G | |||
|Antique green | |||
|aka antique sparkle (is not green!) | |||
| | |||
|- | |||
|} | |||
=== Opaque === | |||
{| class="wikitable sortable" width=90% | |||
|- | |||
! width=50px|Stock Number | |||
! Colour | |||
! Properties | |||
! Reactions | |||
|- | |||
|L1200 | |||
|White | |||
| | |||
| | |||
|- | |||
|L2201 | |||
|Soft violet | |||
| | |||
| | |||
|- | |||
|L2207 | |||
|Iris violet | |||
| | |||
|Reduces to metallic | |||
|- | |||
|L3018 | |||
|Middle blue | |||
| | |||
| | |||
|- | |||
|L3206 | |||
|Iris dense blue | |||
| | |||
|Reduces to metallic | |||
|- | |||
|L4010 | |||
|Iris green | |||
| | |||
|Reduces to metallic | |||
|- | |||
|L4016 | |||
|Beryl green | |||
| | |||
| | |||
|- | |||
|L4205 | |||
|Middle green | |||
| | |||
| | |||
|- | |||
|L4207 | |||
|Light green | |||
| | |||
| | |||
|- | |||
|L5210 | |||
|Opal yellow | |||
| | |||
| | |||
|- | |||
|L6116 | |||
|Lipstick | |||
| | |||
| | |||
|- | |||
|L6208 | |||
|Iris orange | |||
|aka raku | |||
|strikes to multicolour (also reduces to metallic) | |||
|- | |||
|L6210 | |||
|Magic | |||
| | |||
|strikes to multicolour | |||
|- | |||
|L6212 | |||
|Dark red | |||
| | |||
| | |||
|- | |||
|L6213 | |||
|Strawberry | |||
| | |||
| | |||
|- | |||
|L6214 | |||
|Opal orange | |||
| | |||
| | |||
|- | |||
|L6215 | |||
|Light red | |||
| | |||
| | |||
|- | |||
|L6219 | |||
|Opal raspberry | |||
| | |||
| | |||
|- | |||
|L7205 | |||
|Caramel | |||
| | |||
|reduces to metallic | |||
|- | |||
|L7206 | |||
|Scarlet brown | |||
| | |||
| | |||
|- | |||
|L6209 | |||
|Multicolour | |||
| | |||
|strikes multicolour green-blue | |||
|- | |||
|L6218 | |||
|Flamingo | |||
| | |||
|reduces to metallic | |||
|- | |||
|L7202 | |||
|Porcelain | |||
| | |||
| | |||
|- | |||
|L6221 | |||
|Lilac | |||
| | |||
| | |||
|- | |||
|L6202 | |||
|Multicolour dark | |||
| | |||
|strikes multicolour green-blue-purple-red | |||
|- | |||
|} | |||
=== Mystics and Pearls === | |||
These have a shampoo-like sheen, can be semi-translucent and variegated colour. | |||
{| class="wikitable sortable" width=90% | |||
|- | |||
! width=50px|Stock Number | |||
! Colour | |||
! Properties | |||
! Reactions | |||
|- | |||
|L201 | |||
|Mystic violet | |||
| | |||
| | |||
|- | |||
|L301 | |||
|Mystic blue | |||
| | |||
| | |||
|- | |||
|L401 | |||
|Mystic green | |||
| | |||
| | |||
|- | |||
|L501 | |||
|Mystic yellow | |||
| | |||
| | |||
|- | |||
|L502 | |||
|Mystic orange | |||
| | |||
| | |||
|- | |||
|L601 | |||
|Mystic pink | |||
| | |||
| | |||
|- | |||
|L605 | |||
|Mystic red | |||
| | |||
| | |||
|- | |||
|L701 | |||
|Mystic beige | |||
| | |||
| | |||
|- | |||
|L801 | |||
|Mystic grey | |||
| | |||
| | |||
|- | |||
|L803 | |||
|Mystic grey blue | |||
| | |||
| | |||
|- | |||
|L201S | |||
|Pearl violet | |||
| | |||
| | |||
|- | |||
|L601S | |||
|Pearl pink | |||
| | |||
| | |||
|- | |||
|L701S | |||
|Pearl beige | |||
| | |||
| | |||
|- | |||
|} | |||
<!-- Please leave this at the bottom --> | |||
[[Category:Types of Glass]] | |||
Latest revision as of 15:41, 8 December 2010
Reichenbach produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenbach 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down. Reichenbach also produce a range of CoE92 glass rods and frits, many of which are either reactive or reducing colours.
Reichenbach colours and stock numbers
Transparent
| Stock Number | Colour | Properties | Reactions |
|---|---|---|---|
| L1011 | Crystal | clear | |
| L1012 | Crystal soft | soft clear | |
| L2011 | Violet reddish | ||
| L2012 | Gold violet | more violet than rubino | |
| L2013 | Gold ruby light | ||
| L2015 | Pink lady | ||
| L4015 | Antique | aka antique clear, is greenish | |
| L5010 | Silver brown | silver reduction glass | |
| L6015 | Garnet red | ||
| L6027 | Rosalin | ||
| L7003 | Amber | ||
| L9202 | Black | ||
| L5011 | Dark silver brown | silver reduction glass | |
| L9203 | Deep black | may reduce metallic | |
| L1012B | Ocean | blue with sparkles | |
| L1012G | Antique green | aka antique sparkle (is not green!) |
Opaque
| Stock Number | Colour | Properties | Reactions |
|---|---|---|---|
| L1200 | White | ||
| L2201 | Soft violet | ||
| L2207 | Iris violet | Reduces to metallic | |
| L3018 | Middle blue | ||
| L3206 | Iris dense blue | Reduces to metallic | |
| L4010 | Iris green | Reduces to metallic | |
| L4016 | Beryl green | ||
| L4205 | Middle green | ||
| L4207 | Light green | ||
| L5210 | Opal yellow | ||
| L6116 | Lipstick | ||
| L6208 | Iris orange | aka raku | strikes to multicolour (also reduces to metallic) |
| L6210 | Magic | strikes to multicolour | |
| L6212 | Dark red | ||
| L6213 | Strawberry | ||
| L6214 | Opal orange | ||
| L6215 | Light red | ||
| L6219 | Opal raspberry | ||
| L7205 | Caramel | reduces to metallic | |
| L7206 | Scarlet brown | ||
| L6209 | Multicolour | strikes multicolour green-blue | |
| L6218 | Flamingo | reduces to metallic | |
| L7202 | Porcelain | ||
| L6221 | Lilac | ||
| L6202 | Multicolour dark | strikes multicolour green-blue-purple-red |
Mystics and Pearls
These have a shampoo-like sheen, can be semi-translucent and variegated colour.
| Stock Number | Colour | Properties | Reactions |
|---|---|---|---|
| L201 | Mystic violet | ||
| L301 | Mystic blue | ||
| L401 | Mystic green | ||
| L501 | Mystic yellow | ||
| L502 | Mystic orange | ||
| L601 | Mystic pink | ||
| L605 | Mystic red | ||
| L701 | Mystic beige | ||
| L801 | Mystic grey | ||
| L803 | Mystic grey blue | ||
| L201S | Pearl violet | ||
| L601S | Pearl pink | ||
| L701S | Pearl beige |