Author Topic: Cupcake Beads  (Read 3174 times)
0 Members and 1 Guest are viewing this topic.
Rachel B
Forum Member
***
Posts: 100



WWW
« on: June 08, 2008, 05:26:38 PM »

Does anyone have or know of tutorial for making beads in the shape of cupcakes please?
Logged

flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #1 on: June 08, 2008, 05:29:25 PM »

hi rachel,
have you looked on the foodbead swap link?
sure there were some cakes on there, might give you an idea  who to pm,
goodluck , sandy
Logged

beads-on-toast
Forum Member
***
Posts: 214

Dichroic Diva


WWW
« Reply #2 on: June 08, 2008, 06:31:18 PM »

i make them like this -

1. make a wide cone shape (that's the paper case of the cake)
2. add on the top white whippy top.
3. Add ridges to the base with a razor tool to look like a cake paper
4. decorate with stringer for sprinkles
Logged

Billie
Rompin', stompin'
Forum Member
*****
Posts: 602



WWW
« Reply #3 on: June 09, 2008, 04:49:40 AM »

Mmmmmmmmmmmm  Grin Grin
Logged

Rachel B
Forum Member
***
Posts: 100



WWW
« Reply #4 on: June 09, 2008, 05:27:30 AM »

Oooo, thanks again Anna! Cheesy