Main Menu

effetre aqua

Started by stephanie, April 12, 2008, 01:36:20 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

stephanie

I love effetre Aqua, but it seems to frazzle easily, especially where it meets an opaque glass. Any suggestions?
My 'seconds' box is full of this problem!

♥♥Tan♥♥

Try working a bit higher up in the flame, its getting too hot, if an area is bubbly hold it in the flame a bit longer and it should get rid of the worst of it

stephanie

okay, I'll try to be more disciplined about where I work it in the flame. Sometimes the bubbles don't burn off, they get worse, then I try to encase instead...more trouble!
Would you reject a bead because of a bit of pitting? I think I have become super-critical of my efforts. Lots of my beads are just fine and I wouldn't have judged them this harshly if they had been made by someone else, I'd have strung them and put them on...

mad bunny

I was having the same problem, then I wasn't.  I think it was the teal opaque I was having trouble with. 

Do you get a bright sizzling effect?  I thought I had managed to stop it, but yesterday I made a black bead with white spots and it happened on that one. As you say it doesn't seem to dissappear once it's happened and I would put those beads out as seconds.

Working further up the flame does seem to help, but the glass takes longer to melt and form the bead.
Maybe I am being too impatient.  ::)
Practice and Patience really does pay off!  Beads actually looking good  Yippee  :o

stephanie

yes, teal too, now that I think of it. It's so unfair! The ratio of 'good' beads versus 'seconds' is too low for all that effort, but I think I am trying to run before I can really walk and I have to be patient in more ways than one.

♥♥Tan♥♥

Pitting isnt a bad thing as long as its what your aiming for, you cant cover up a crappy bead as a happy accident though,

Dont be impatient, you've only just started, you cant expect to turn out perfect beads right away, you have to practice

stephanie

yes, I feel like an ancient bead maker, but I don't even have a year of actual bead making under my belt. I must remember that! 

♥♥Tan♥♥

Try an organic bead and make the pitting work in your favour

Vicki

I've had this problem with certain colours that I didn't have previously, I've tried every torch setting & melting the glass in slow motion, but no joy at all...I've even had to take turquoise spacers of my website because of this....I have no idea whats different to before :(  maybe if we knew the answer it would help both of us...unfortunatly I haven't a clue!

stephanie

Thanks Tan, for trying to help, & Vicki for me not being the Only One : )
Min

Shirley

I find it is really obvious with certain frits. I've got some copper blue frit and every time I so much as look at it it starts to fry. Just made a really nice focal and it's got some pitting where the silver leaf I used has played silly B's. Looks effective though, so I'll take Tan's advice and call it organic :D
Val Cox Frit - Thai and Bali Silver 

Vicki

its just odd though as I never had any problem a few months back, its not the propane either as I changed recently :-\  & no Min your rarely alone in a crisis ;) :D

stephanie

Quote from: Shirley on April 12, 2008, 04:58:25 PM
I find it is really obvious with certain frits. I've got some copper blue frit and every time I so much as look at it it starts to fry. Just made a really nice focal and it's got some pitting where the silver leaf I used has played silly B's. Looks effective though, so I'll take Tan's advice and call it organic :D

your 'Blossom Tree' bead is lovely : )

Shirley

Val Cox Frit - Thai and Bali Silver 

fionaess

Quote from: Vicki on April 12, 2008, 03:10:48 PM
I've had this problem with certain colours that I didn't have previously, I've tried every torch setting & melting the glass in slow motion, but no joy at all...I've even had to take turquoise spacers of my website because of this....I have no idea whats different to before :(  maybe if we knew the answer it would help both of us...unfortunatly I haven't a clue!

I am having terrible problems with my Effetre dark turquoise, burning, pitting and it seems to reduce just by looking at the flame.. it's so bad that I'm not using the stuff.. and I have 1/2 kilo., I know for certain that my last dark turquoise from Tuffnells was fine, this batch is terrible. My light turquoise is ok though.


If it's got a hole, it's a bead !