Hartofglass

Has anyone used Reichenbach Gold Violet?  Is it good to work with?  Does it behave like Rubino Oro?  I'm very new to using these sorts of glass and would appreciate your experience. Thanks!

helbels

It's a nice pinky purple transparent - not fussy to work with like Rubino, and can take the heat.  However, not as nice a pink as Rubino, sadly.

Hartofglass

Thanks for your advice. As I'm new I'm a bit scared of Rubino Oro though I have got some rods so I must persevere! 

theflyingbedstead

Quote from: helbels on November 15, 2014, 02:43:13 PM
It's a nice pinky purple transparent - not fussy to work with like Rubino, and can take the heat.  However, not as nice a pink as Rubino, sadly.

Now I disagree! :P  It is a beautiful pink, and goes wonderfully with teal and ink blue. Not as "Barbie" as rubino! One of my favourite colours and it plays nicely  ;D
Charlotte x

Princess Peggy (Priscilla McGirr)

It seems to vary from batch to batch, some of the rods I have had from Tuffnells in the past have been a really good dark pink, but the last ones are more dull. 
Pris