Main Menu

Reichenbach dense black

Started by cbeadies, June 10, 2013, 07:50:35 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

cbeadies

I thought this blog post may be of interest to anyone looking for the best black for stringer work, etc

http://chestnutridgedesigns.com/sections/blog/blog.aspx

Tuffnells sell a Reichenbach Deep Black...does anyone know if this is the same glass as Dense Black?

Shirley

I don't know for sure but I would suspect it's the same thing, unless they are different COE. I use the deep black 104 from Tuffnell's for my black stringer work. It is the best I have used, and I've tried lots.
Val Cox Frit - Thai and Bali Silver 

DragonArtGlass

Thanks for sharing this... have you looked at other entries here?
There seems to be lots of useful information and tips.

Jolene

It's absolutely brill for stringer work but it also does some pretty cool crazy stuff over a couple of CiM colours and Mystic Red too http://www.kitzbitzartglass.blogspot.co.uk/2012/10/reichenbach-deep-black-stringer.html

Kaz

Make sure you buy the "deep black" and not the black as the black spits and sputters and silvers up in the flame.
Deep black also has some very interesting effects with silver glass often changing colour completely.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Emma @ Tuffnell Glass

Yes its the same. I think it depends on what translation site Martin used  ;)
but I use the deep black and its brilliant!

Shirley

I have it in my Frit shop too.
Val Cox Frit - Thai and Bali Silver