Author Topic: Melting Bullseye to a pre-determined size - No mould method?  (Read 28910 times)
0 Members and 1 Guest are viewing this topic.
Barnacle Bay
Forum Member
****
Posts: 250


I'm Just a Little Bit Potty


« on: May 21, 2013, 07:23:19 AM »

Hi Folks,

I am wondering if there is a method or rule of thumb when melting bullseye to finish up at a predetermined finished size in a kiln, i.e want a finshed pendant to end up at a specific size like 25mm x 25mm, without using a mould, which will fit into a pre-made bezel/cab setting?

I am asuming it will depend on the thickness of the glass and size cut, but I am also wondering if there is a expected expansion formula to the pre-cut size?  

Thank you in advance.

Lou
Logged
Hamilton Taylor
Hamilton Taylor Studio - Flameworked and Kilnformed Glass
Forum Member
****
Posts: 254


Flameworked and Kilnformed Glass


WWW
« Reply #1 on: May 21, 2013, 07:49:43 AM »

A chunk of glass in the kiln, taken to full fuse, will form a puddle about 6mm thick. This is due to the surface tension of the molten glass.
If you want a specific design, arrange your glass so that it is consistently 6mm thick, and it should fuse 'in place', changing little as it fuses.
Unfortunately, absolute accuracy is not guaranteed, so a little coldworking is often necessary if you want to fit a pre-made bezel.

There is no expansion to take into account - you end up with the same volume after fusing as you had before.

Sean
Logged

Barnacle Bay
Forum Member
****
Posts: 250


I'm Just a Little Bit Potty


« Reply #2 on: May 21, 2013, 08:02:50 AM »

Thank you ever so much for that Sean, but could you explain coldworking  - is it allowing the kiln to cool inbetween the fusing/heating process?
Logged
Hamilton Taylor
Hamilton Taylor Studio - Flameworked and Kilnformed Glass
Forum Member
****
Posts: 254


Flameworked and Kilnformed Glass


WWW
« Reply #3 on: May 21, 2013, 10:51:19 AM »

Sadly not! It's using grindy-things such as diamond pads and dremels to shape, clean and polish glass.

Download an overview here

Sean
« Last Edit: May 21, 2013, 11:24:03 AM by Zeldazog » Logged

Nicknack
Forum Member
****
Posts: 472

To bead, or not to bead? ..... stupid question!


« Reply #4 on: May 21, 2013, 10:53:16 AM »

Cold working is grinding, smoothing and polishing the cold piece after it's come out of the kiln.  A bit like lapidary (stone polishing).  if you follow Sean's instructions you shouldn't have to do much, and probably wouldn't need to polish the bits that would be covered by the bezel.

Nick
Logged
Barnacle Bay
Forum Member
****
Posts: 250


I'm Just a Little Bit Potty


« Reply #5 on: May 21, 2013, 10:56:00 AM »

Sadly not! It's using grindy-things such as diamond pads and dremels to shape, clean and polish glass.

Download an overview here

Sean

SUPERB replys - thank you again  Smiley  I do have Dremels & Grindy things thanks to hubbys vast emporium of gadgets!

Oh No - Link not working Sean  Shocked
« Last Edit: May 21, 2013, 10:58:39 AM by Mr & Mrs Quilla » Logged
Zeldazog
My name's Dawn, I'm an
Administrator
*******
Posts: 1048


I'm free, to do what I want...♪♪♪


« Reply #6 on: May 21, 2013, 11:24:35 AM »

Modified Sean's link, it should work now.
Logged

Barnacle Bay
Forum Member
****
Posts: 250


I'm Just a Little Bit Potty


« Reply #7 on: May 21, 2013, 12:30:57 PM »

Modified Sean's link, it should work now.

Yes it does thank you for fixing it  Smiley
Logged
Flyingcheesetoastie
On Golden Wings of Cheddar...
Forum Member
****
Posts: 361


Mostly making glass...


WWW
« Reply #8 on: May 21, 2013, 01:18:42 PM »

 Cool Just stealing that link for future student handouts....
Logged

Barnacle Bay
Forum Member
****
Posts: 250


I'm Just a Little Bit Potty


« Reply #9 on: May 21, 2013, 01:27:54 PM »

Cool Just stealing that link for future student handouts....

Good bit of info - I just need to find out about fine grade kit for our tumbler that has been sitting idle in the garage - I feel it may now come in use  Smiley
Logged
Hamilton Taylor
Hamilton Taylor Studio - Flameworked and Kilnformed Glass
Forum Member
****
Posts: 254


Flameworked and Kilnformed Glass


WWW
« Reply #10 on: May 21, 2013, 03:33:01 PM »

Oops, sorry about the link, I was in a rush...
Logged

Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.059 seconds with 18 queries.