MONTHLY THEME CHALLENGE - February

Started by Krysia@No98, February 04, 2013, 05:32:23 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

katherinem

I love everyone's beads! and they're all so different!

Organic really isn't something I've tried, I think maybe I need to learn a bit of restraint, especially with the silver foil  :) Here's my effort, front and back of the same bead (apologies for the dodgy photos)


Organic 1 by katherinem2012, on Flickr


Organic 2 by katherinem2012, on Flickr

GaysieMay

Loving all these beads - stoneground is one of my favourite glasses too.  Here are my organic seascape beads - I used a picture Lotti sent me as the inspiration


Organic Seascape beads - sold by GaysieMay, on Flickr

Sorry picture is so appalling but we haven't seen the sun for a while!  ::)
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

jeannette

Beads are all really yummy!

Phew - been in the making for weeks! Eventually finished it last night. It's an idea from the Bullseye tip sheets.


P1000298 by Jeannette Copeland, on Flickr



P1000299 by Jeannette Copeland, on Flickr

Calico Cat

Decided to play with my new parallel mashers :-)

This is sediment, ivory and avocado




Plus a beach bead using sediment and ink blue



Decided I like sediment . . . .


Watch this space for new Etsy shop . . .

Kalorlo

Katherine, I really like that bead!
Jeannette: that is fab!

ETA: I love sediment  :)

nete


marklaird

Love them all, but I really love the effect of the sediment glass. What is it, where can I get some?

Mark

Calico Cat

Quote from: marklaird on February 24, 2013, 07:13:49 PM
Love them all, but I really love the effect of the sediment glass. What is it, where can I get some?

Mark

Sediment is an Effetre glass - not sure if it's available in the UK - but if you would like a rod to try PM me your address and I'll fling one in your direction next weekend (I'm working away all this week).

Carole


Watch this space for new Etsy shop . . .

Trudi

Ohh Jeanette - you finally finished the plate .... it looks amazing. I will have to pop round for close inspection!

Loving the beads everyone ... I've been making quite a few organics since this challenge popped up. Lots of inspiration on here!

Yellow friend

Yes what a wonderful plate Jeanette :)

Shelia
www.crocosmiajewellery.com
www.crocosmiajewellery.etsy.com

SueP


jeannette

Thanks all - lovely of you to say.
It's gone to its new home- I hope they like it :)


Donna@Rockin' Beads

Ooo, there are some lovely beads in here.
I don't normally do organics but my mum asked for something to match in with her lapis and I'm quite pleased with how this one turned out...

Lapis Lazuli Lookalike by Rockin' Beads, on Flickr

Skyblue