Started by jammie, June 02, 2012, 09:35:37 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

jammie

Im using a nugget press for the first time and getting there, but has anyone any tips on getting the ends neat, some are great, some have flat at one end and a more dimpled end at the other?

Margram

Have you tried the plasticine trick to see how much glass you will need before pressing? - and marking the mandrel with an indelible pen for your footprint? :)
Marg x  Etsy Flickr My blog

jammie

Not tried that no, was thinking I just needed a little more glass at one end though right enough!  :)