On Tuffnells website, marmorin glass looks silvery grey with streaks in it.  I rather fancied this.  I cannot get it to look anything like the picture!  It is pale ble in the rod and very pretty - it will stay like that if you don't do anything else with it.  I have tried striking and reducing.  All I can get is a pale blue base with muddy brown splotches, which disappear if it is warmed again.  Anyone know if there are any tricks to getting anything more out of this glass?  Thanks  :)
Turner Rowe Glass Art

Vikkijayne

I wish i knew the answer! I got some of this glass yesterday so I hope someone offers up some good advice, cos as you said it looks nice on tuffnels website

amareargentum

I'm sure I got some Marmorin from Frantz some while back. If I am remebering correctly then my rods are grey not blue. Unfortunately they stayed grey and I couldn't get them to do anything else.

Princess Peggy (Priscilla McGirr)

I'm just as puzzled as the rest of you, and quite honestly I think it is a swiz, think that's a word from the beano comic, anyway no sign of the lovely gold splodges, just dirty brown which look as if you've accidentaly burnt the glass...anyone know the secret to this glass?
Pris
My Website http://www.dancingwithglass.co.uk  My Etsy http://www.etsy.com/shop/princesspeggy01
My Facebook page: https://www.facebook.com/DancingwithglassLampwork

Lakelady

There was a post on the interweb somewhere - a person got it to work.  I will have a look and see if I can find it again - the post was the reason why I bought it and tried reducing it...now tried everything but nothing but the brown splodge on a rather aqua pale blue! 
Turner Rowe Glass Art

k00m

Here's DragonJools's test of it, which seems to imply that reducing is the key.
And Coloraddiction has tested the light version which seems to strike.  ???
Unfortunately Mind Melt doesn't seem to have tested it yet, which is a pity, as I really like the way she tests.

I'm not sure if that helps at all  ::). It might reduce or it might strike or it might do both! Looks like its a bit of a mystery glass.
- Kerra -

Lakelady

It was the DragonJools one that I saw.  Might try encasing on clear to see what happens.  I have got it to a pale blue with greenish striations, so there is something there....will have to persevere... :-\
Turner Rowe Glass Art

Pandanimal

I love that mind melt blog.
I spent hours on it last night going "Ohhh!" and "Ah ha!"
Shame she hasn't done marmorin I got some of that last week. along with light and dark zucca and green metalic copper which is just soo nice.  ;D

tomcat

one from me on marmorin, i melted it and shaped it into a lentil in a press - then reheated to melt again totally and added more glass - then reshaped to a lentil and then reduced it  - mind you its on a hot head so thats a reducing flame all the time reallly



I quite like it and will see if i can get a set together - but the real question is - what happens when it is annealed ?
Mark - Blog - http://beadsbeerandphotos.blogspot.co.uk/
Life is not a game - its THE game, so play it like you mean it
A Long time ago in Egypt cats were worshipped as Gods, cats have not forgotten this !

Ness

I really like it, try using it as a base for silver glass.

(I have the grey stuff, from Frantz yonks ago)

Pauline

Quote from: tomcat on December 12, 2011, 06:46:37 PM
one from me on marmorin, i melted it and shaped it into a lentil in a press - then reheated to melt again totally and added more glass - then reshaped to a lentil and then reduced it  - mind you its on a hot head so thats a reducing flame all the time reallly



I quite like it and will see if i can get a set together - but the real question is - what happens when it is annealed ?

Bring it over and we can try it!

Lakelady

There was a reply from Dragon Jools and she couldn't rememer how she got it but hers is closer to the paddle colour than any other I have seen!
Turner Rowe Glass Art

Oenone

Quote from: Pandanimal on November 24, 2011, 02:01:03 PM
I love that mind melt blog.
I spent hours on it last night going "Ohhh!" and "Ah ha!"
Shame she hasn't done marmorin I got some of that last week. along with light and dark zucca and green metalic copper which is just soo nice.  ;D

Thank you k00m and Pandanimal for the nice feedback about my blog!  My blogger stats directed me to this thread, since you've generated a little bit of traffic to my site by talking about it.

I think I have reviewed the green metallic copper - Frantz Art Glass calls it Neptune, so that's what I've called it on my blog.  Aren't the different names for things confusing? I haven't tried the Zuccas, but I have a little Marmorin so I'll put that on my list of things to try in the new year when I get back to the torch.

My blog hasn't received any updates in the last couple of months because I've been moving and under crazy work deadlines... and my torch is in the garage and it's been pretty cold here, but I'll be headed into Vancouver to buy torch time in January.  My updates will be sort of spaced out until things warm up here and I can torch at home, but I can promise a post or two in January, and probably a few more in February.

If you ever have requests for me to include in my testing schedule, just leave me a comment on my blog and I will try to accomodate it :)

Hope everyone has a great holiday season!
Melanie

awrylemming

Wonderful blog Melanie  ;D  Merry Christmas to you too.

Oenone

Just wanted to let everyone know that I managed to get some test beads with Marmorin posted on my blog :)
http://melanie-graham.blogspot.com/2012/03/test-results-marmorin.html