Hi

Just wondered if anyone knows about some new CIM colours coming out?  I was browsing Beverley Hicklin's Make Glass Beads new website and she mentioned CIM "Mint Lozenge" and "Indigo".  I've just visited CIM's website and they are there, but nobody in the UK seems to have them yet?

Then I got very excited as on the CIM site I spotted two pinks I'd sell a kidney for ...  "Razzleberry" and a streaky "Crane" pink?  Does anybody have any insider info or know where I can buy some of these two pinks please?

mand x

Calico Cat

Not even available from Frantz yet . . . .


Watch this space for new Etsy shop . . .

Kalorlo

Razzleberry's come and gone, I think. Frantz had it all for a bit.

princess pink

i've just ordered some of the new limited mint lozenge and indigo from frantz, will tell you what they're like. Razzleberry really not that great too be honest x

awrylemming

I have one stick of Razzleberry (half now) that Shahlaa gave me in the first place.  Actually I really like it, but it's now impossible to get yer paws on.  You could harass the lovelies at CIM  ;)  Mint lozenge seems nowt special, indigo much the same, they're sitting in the stash.