Lotti

OOh, very interesting, slightly different from their other glass. :)

The Tartan Trout

Quote from: Lotti on August 09, 2011, 04:55:52 PM
OOh, very interesting, slightly different from their other glass. :)

doubt it...I bet I could still make them turn out a lovely poo/beige colour :)

Blue Box Studio

They are interesting.  I wonder if they are easier to use than normal DH glass?
Sue
Website ~ Etsy ~ Blog ~ Flickr

turtle

will they be available over here or do you need to order from across the pond?
Chris

kathsd

oooerrrr! I likes them lots (I think my bank card's just run off to hide!!thankfully! :D)
kath

Shirl

I think some will have to be added to my list when I go to America :)

Fruddy

Quote from: turtle on August 09, 2011, 07:19:57 PM
will they be available over here or do you need to order from across the pond?

Sorry Turtle, but the test batches and such like from DH are across the pond.... they don't sell them over here....

Chameleon

ooo some lovely ones in there, and some original Terra  ;D ;D

turtle

Do you get customs grief if you order from the states?
Chris

Sarah A

Quote from: turtle on August 10, 2011, 08:30:56 AM
Do you get customs grief if you order from the states?

I placed a small order (for seconds) a couple of months ago which came in under customs charges worked out cheaper than buying non seconds over here and arrived in less than 2 weeks!

Fruddy

Quote from: turtle on August 10, 2011, 08:30:56 AM
Do you get customs grief if you order from the states?

It depends on the value of your order Turtle.... if you were to order say just one batch of the DH for $20.00 then you would get away without the Customs ransoms etc., but any more than this and you would get snagged with it, unfortunately.

turnedlight

Thanks for the heads up, i saw it whilst on my hols and decided to treat myself  ;D
I just received them, Doesn't quite look like my original terra rods, which are thin, dark brown outside and very stripey, these look a bit like ekho but stripey inside - will have a go and keep you posted!
kathryn

Fruddy

Quote from: turtle on August 10, 2011, 08:30:56 AM
Do you get customs grief if you order from the states?

Interestingly, despite my earlier reply Turtle, I have just picked up my box of DH Test Batches from the Post Office and it has managed to slip through the Customs net this time, despite the value of the contents being over £20.00.....

I think that's the first time that has ever happened!!!

turnedlight

How do you know if it has been caught? My package doesn't have anything from customs on the outside, do you think mine slipped through too?
kathryn