Main Menu

Lace effects?

Started by Ant, July 20, 2011, 10:59:56 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Ant

Following my recent post I've managed to make some lovely lacey beads using Hades stringer on Ivory (will hopefully post photos shortly).  Do any of you know of any other colours that react the same way under intense heat?  I quite fancy having a go at similar beads in other colours.

SilverGems89

You usually get a much better effect on transparent than opaque glass but it's just a case of trial and error for most of them to find out if they work!

MadelineBunyan

not many colours do the webbing thing
I think mosaic green does it, but I may be wrong, check ou the list of colours and properties on the wiki

however, the black looks fab on sooo many different backgrounds!