pearl biege help.

Started by Shirl, July 20, 2011, 10:37:56 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Shirl

Thanks Sue I will take you up on your offer.
I will make 2 small beads together on the same mandrel and put one in my kiln, and let you have the other then we will know for sure  :)

julieHB

I wonder if there's a chance it's silver fumes that have caused it to darken.

At what temperature do you anneal? I would certainly try to anneal with no silver glass in the kiln at the same time.
Julie xx

                           My Webbie - My Flickr

awrylemming

Well you know my address Shirl, pop it in the post and I'll batch it with my non silver beads - I always do them separately, as I had problems with pinks fuming in the kiln.

Shirl

Thanks Sue.

I will take advice and anneal my silver glass separately from now on. :)