Frit-Happens !
May 14, 2021, 10:25:45 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: 1 2 3 [4]
  Print  
Author Topic: A FREE tutorial  (Read 6623 times)
0 Members and 1 Guest are viewing this topic.
Veebee
Superglassyfrittylisticgirlmakes beadsatrocious!
Forum Member
****
Posts: 392


Serial HotHead on bulk user and glass murderess.


WWW
« Reply #45 on: June 12, 2011, 06:44:54 AM »

Thank you Miriam, it's a great tutorial!
Logged

Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/
Corinne Lacy
Forum Member
*
Posts: 49


« Reply #46 on: June 12, 2011, 10:57:13 AM »

Hi, just tried this link and the download wouldn't work, should I try again or email you directly?

Corinne
Logged
Miriam
Forum Member
**
Posts: 65



WWW
« Reply #47 on: June 12, 2011, 12:18:00 PM »

I just checked and the link is working fine.

Please if you have any trouble, reply on the email or contact me on my website. It is so difficult to keep up with fora all over the world. I won't forget you when you email me, because my inbox is my memory. ;-)
Logged

groetjes Miriam


Blog | Website | Colorcharts | Glasss
Shirl
Forum Member
****
Posts: 371


« Reply #48 on: June 14, 2011, 10:47:23 AM »

Wooohooo.

Just got this out of my kiln and its the brightest bead I have ever made! I didnt have the correct orange so just used what I had, and it has turned out quite well I think Smiley It seems to glow!

Logged

turnedlight
Forum Member
*****
Posts: 637

Kathryn


WWW
« Reply #49 on: June 14, 2011, 11:07:56 AM »

That's lovely, was it still a transparent orange, or was it opaque like it looks at the end?
Logged

kathryn
Shirl
Forum Member
****
Posts: 371


« Reply #50 on: June 14, 2011, 11:13:20 AM »

No, I didnt have any transparent orange so used opaque, the little sample in at the end, it was richenbach opal orange
Logged

turnedlight
Forum Member
*****
Posts: 637

Kathryn


WWW
« Reply #51 on: June 14, 2011, 11:17:21 AM »

Ok, cool! I might have a go tomorrow, I have some of that orange! I had go the other day, but the rod turned out to be trans red and it went too dark. Roll Eyes
Logged