Title: A FREE tutorial Post by: Kaz on June 09, 2011, 03:59:40 AM Miriam is offering this free tutorial on her website
http://www.miriamsteger.nl/blog/2011/06/09/een-shocking-pink-tutorial-gemaakt/ In case you haven't spotted it! Kazx Title: Re: A FREE tutorial Post by: paintboxcrafts on June 09, 2011, 04:05:07 AM I have just downloaded it, but it was an empty file and didn't work.
Did it work for you? Cathy Title: Re: A FREE tutorial Post by: Kaz on June 09, 2011, 04:06:26 AM I've not had my email link yet but will contact Miriam and let her know if I have problems!
Kazx Title: Re: A FREE tutorial Post by: awrylemming on June 09, 2011, 04:30:51 AM Mine was emailed immediately and no problems. Did you follow the link and leave your name? :-\
Title: Re: A FREE tutorial Post by: paintboxcrafts on June 09, 2011, 04:45:00 AM Miriam has kindly sent it again, the first file that arrived was called 'noname' and had a size of 0K,
I should have noticed that it wasn't going to work! Title: Re: A FREE tutorial Post by: awrylemming on June 09, 2011, 05:01:46 AM Miriam has kindly sent it again, the first file that arrived was called 'noname' and had a size of 0K, I should have noticed that it wasn't going to work! ;D ;D Title: Re: A FREE tutorial Post by: dinah46 on June 09, 2011, 05:10:44 AM I don't get anything either, just a message saying there's an attachment but no attachment to open - curious ???
Title: Re: A FREE tutorial Post by: Miriam on June 09, 2011, 05:25:58 AM My webserver is going crazy!!! So many people try to download the tutorial at the same time. The server can't handle this and sends out empty attachments.
Please reply to the email that is been send and I will send you the file by hand. Be patient, I am not at my computer the whole day. ;-) Title: Re: A FREE tutorial Post by: Louise Menzies on June 09, 2011, 05:51:39 AM Server is very busy it wont even let me download or request it :).... I will come back later x
Title: Re: A FREE tutorial Post by: dinah46 on June 09, 2011, 05:55:18 AM Thanks Miriam, received mine from you now :)
Title: Re: A FREE tutorial Post by: jammie on June 09, 2011, 06:11:04 AM Its saying come back later on ....so i will. :)
Title: Re: A FREE tutorial Post by: Miriam on June 09, 2011, 06:51:21 AM It is back online!!
The demand on the server is so high, I might shut down the download later on for a short time. Title: Re: A FREE tutorial Post by: jammie on June 09, 2011, 06:59:26 AM I filled it in but the email cam back without an attachment, will I try again later?
Title: Re: A FREE tutorial Post by: Miriam on June 09, 2011, 07:01:58 AM Jammie, please reply to the email and I will send the tutorial by hand.
Title: Re: A FREE tutorial Post by: jammie on June 09, 2011, 07:03:46 AM Done that, thanks so much :)
Title: Re: A FREE tutorial Post by: Angie on June 09, 2011, 07:56:33 AM Thanks Miriam, it looks great.
Title: Re: A FREE tutorial Post by: Jolene on June 09, 2011, 07:58:39 AM It's a fab tut, thank you Miriam
Jo x Title: Re: A FREE tutorial Post by: jammie on June 09, 2011, 08:42:23 AM Got it now Miriam, thanks very much! :)
Title: Re: A FREE tutorial Post by: MadelineBunyan on June 09, 2011, 08:55:43 AM got mine! thanks! such lovely happy heart beads you've made!
Title: Re: A FREE tutorial Post by: Trudi on June 09, 2011, 12:02:14 PM Ohhh I've sent for one - can't wait.
It's very generous of you Miriam - thank you. And thanks to Kaz for posting the link! Title: Re: A FREE tutorial Post by: turnedlight on June 09, 2011, 12:48:22 PM Thank you! The pink is soo pink! ;D
Title: Re: A FREE tutorial Post by: Lush! on June 09, 2011, 01:15:21 PM That's the second time I've heard striking orange mentioned this week ... interesting ... :D
Title: Re: A FREE tutorial Post by: julieHB on June 09, 2011, 02:21:59 PM Lovely tutorial, wonderful pink beads, Miriam!
Had a little play today, and although I didn't achieve Miriam's shocking pinks I am quite pleased (I know what I did "wrong" ;)) : (http://farm4.static.flickr.com/3328/5814845907_cb08537e58.jpg) (http://www.flickr.com/photos/juliehb/5814845907/) Ringtop Purple Summer (view 2) (http://www.flickr.com/photos/juliehb/5814845907/) by JulieHB (http://www.flickr.com/people/juliehb/), on Flickr (sorry to those who have seen it elsewhere!) Title: Re: A FREE tutorial Post by: dangerousbead on June 09, 2011, 03:26:09 PM thanks for the heads up Kaz and thank you Miriam, planning a long awaited play day on Saturday so Ill have a go then.
Title: Re: A FREE tutorial Post by: Dragonfire Glass on June 09, 2011, 03:34:54 PM that's rather nice without pinks Julie ;D
Title: Re: A FREE tutorial Post by: julieHB on June 09, 2011, 03:37:57 PM Thanks, Collette ;D There are actually a lot of pinks in there, but it was a bit camera-shy :D ;)
Title: Re: A FREE tutorial Post by: JKC on June 09, 2011, 03:50:09 PM Thanks Miriam, lovely tutorial, also thanks Kaz. Julie, love the cab.
Title: Re: A FREE tutorial Post by: Ilona on June 09, 2011, 04:23:43 PM I have tried twice and it keep getting one that is no name and doesn't work :'( I will try once more.
Title: Re: A FREE tutorial Post by: June on June 09, 2011, 04:30:14 PM That's pretty, Julie :)
Title: Re: A FREE tutorial Post by: Ilona on June 09, 2011, 04:41:51 PM I have given up ::)
Title: Re: A FREE tutorial Post by: cbeadies on June 09, 2011, 05:33:52 PM I have given up ::) don't give up Ilona! I replied to the blank email I received at first, to say I would like a copy, and later on this evening Miriam emailed it again and it opened this time. It looks great! Title: Re: A FREE tutorial Post by: dangerousbead on June 09, 2011, 05:35:33 PM I have given up ::) pm your email and I'll forward it to youTitle: Re: A FREE tutorial Post by: Shirl on June 09, 2011, 05:42:38 PM It wont work for me either :(
Title: Re: A FREE tutorial Post by: Miriam on June 09, 2011, 05:45:11 PM Just send me an email and I will send it to you. I am shutting down the computer now, I need my beauty sleep. ;-) So tomorrow I will send out the tutorials.
Title: Re: A FREE tutorial Post by: Margram on June 09, 2011, 05:52:25 PM Thanks Miriam (and Kaz) :)
Title: Re: A FREE tutorial Post by: Trudi on June 09, 2011, 06:13:20 PM Ohh the tutorial is lovely!!
Title: Re: A FREE tutorial Post by: Trudi on June 09, 2011, 06:13:59 PM Oh ... nearly forgot to say how beautiful your ring topper is Julie .. gorgeous as always!!
Title: Re: A FREE tutorial Post by: LilLizaJane on June 09, 2011, 06:41:15 PM I tried to get your tutorial tonight and I got an empty email in reply! It's obviously a very popular tutorial!
Title: Re: A FREE tutorial Post by: sangemarie on June 10, 2011, 03:23:04 AM I tried to get the tutorial last night and I received an empty file too, but I e-mailed Miriam and it is alredy here this morning, thanks Miriam :) :)
Title: Re: A FREE tutorial Post by: Shirl on June 10, 2011, 05:11:44 AM Thank you Miriam, and Kaz of course. ;D
Title: Re: A FREE tutorial Post by: Louise Menzies on June 10, 2011, 06:03:04 AM Thank You, Patience is a vertu :)
Title: Re: A FREE tutorial Post by: Mand on June 10, 2011, 09:43:46 AM Thank you so much Miriam! ;D ;D ;D
Title: Re: A FREE tutorial Post by: Shirl on June 10, 2011, 10:36:44 AM All I need now is orange. ;D
Title: Re: A FREE tutorial Post by: Trudi on June 11, 2011, 02:37:58 PM The future is bright!
Title: Re: A FREE tutorial Post by: Miriam on June 12, 2011, 06:43:45 AM I have altered the method to get the tutorial. If you put up your name and email address, you will receive an automatic email response with a download link.
Title: Re: A FREE tutorial Post by: Veebee on June 12, 2011, 06:44:54 AM Thank you Miriam, it's a great tutorial!
Title: Re: A FREE tutorial Post by: Corinne Lacy on June 12, 2011, 10:57:13 AM Hi, just tried this link and the download wouldn't work, should I try again or email you directly?
Corinne Title: Re: A FREE tutorial Post by: Miriam on June 12, 2011, 12:18:00 PM I just checked and the link is working fine.
Please if you have any trouble, reply on the email or contact me on my website. It is so difficult to keep up with fora all over the world. I won't forget you when you email me, because my inbox is my memory. ;-) Title: Re: A FREE tutorial Post by: Shirl on June 14, 2011, 10:47:23 AM Wooohooo.
Just got this out of my kiln and its the brightest bead I have ever made! I didnt have the correct orange so just used what I had, and it has turned out quite well I think :) It seems to glow! (http://i1129.photobucket.com/albums/m517/scottam/10cmfocus015.jpg) Title: Re: A FREE tutorial Post by: turnedlight on June 14, 2011, 11:07:56 AM That's lovely, was it still a transparent orange, or was it opaque like it looks at the end?
Title: Re: A FREE tutorial Post by: Shirl on June 14, 2011, 11:13:20 AM No, I didnt have any transparent orange so used opaque, the little sample in at the end, it was richenbach opal orange
Title: Re: A FREE tutorial Post by: turnedlight on June 14, 2011, 11:17:21 AM Ok, cool! I might have a go tomorrow, I have some of that orange! I had go the other day, but the rod turned out to be trans red and it went too dark. ::)
|