Started by Shirl, March 07, 2011, 07:50:02 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Shirl

I just got some of this today to give it a try after seeing it made into some gorgeous dotty beads by Helbels.

I made a small plain bead to test it out and it is quite a pretty pink (I thought it might stay white!)

Is it best used for the whole bead or should it be used on top of a white core?

helbels

I've only used it as a whole bead Shirl, but give it a go over white and see what it does....

cbeadies

 :D I think you've started something Helen! I've just ordered some of this after seeing your lovely beads too!

SueP

Me too managed one pretty pink one and I over worked the next - went white  :(

lyzzydee

I have made beads with this today and the ones I gave a good roasting have come out a beautiful shade of deep pink, the ones I didn't I just made them spacer shape and quick have gone a white with a tinge of pink. Overall I likey!!!