Lauscha - new 104 silver glass compatible formula

Started by sublimekate, December 04, 2010, 09:59:26 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

sublimekate

Lauscha - new 104 silver glass compatible formula

Anyone tried this yet, just ordered myself some, I really love lauscha but it's never been very good, well actually it's been crap with silver glass but this is supposed to be a new formulation??


Jolene

Didn't know about this one, it will be wonderful if it does what it says it will on the tin. Let us know how you go?

Jo x

Tills

I'm not brill on encasing and thought it was me when all my encased over silver cracked, so I bought some of the new compatible Lauscha and so far... No cracks!  ;D

Best of luck!

helenfc

that sounds good, I hadn't heard about it! where did you get it from Kate?

Krysia@No98

-* -  Courage is going from failure to failure with out loosing enthusiasm -*-


Kalorlo

#6
How new? Lauscha clear was reformulated in 2007ish (also when the soft clear came out). I haven't heard anything about another one.

Certainly what I've got is the usual reformulated clear, which is mostly just being called clear now. (Yes, I know, website still getting there!)

It *was* reformulated to make it more compatible with silver glass and other manufacturers' glass in general, and from LE I think people have better luck with it than the soft clear with silver glass, but it's one of those things that some people have problems with and some don't.