Started by helenfc, August 09, 2010, 11:08:05 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

helenfc

A few of us are putting in a frantz order and they have precision 104  ;D ;D ;D
so I know sashas silver is meant to be a bit fab, is there anything else you guys would recommend? They had stopped selling it in the UK by the time I got my set up so any hints/tips would be much appreciated  :-*

Trudi

Hi

Rembrandt is very nice - green like Gaia but much easier to work with - it's a reducer!

helenfc


Kaz

Sacha's silver.
Would have said black pearl but see that it's out of stock - shame!
IMHO none of the precision 104 range is as good as DH. Probably why Martin stopped stocking it - so don't disappoint yourself by ordering tons of the stuff!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Trudi



This was made using shards - looks much better IRL


Where Gaia can be difficult - this one is very easy!

And I guess it's fair to say that many of the other preision colours were difficult to work - but this is good ans so is Sacha's. I think Katherin likes Black Pearl, I have some but haven't really had a good play with it to be fair!

dinah46

Haven't had much success with precision 104 but loved sasha's silver when I first got it. Unfortunately the second lot was nowhere near as good for getting the colours.