Started by BeadyEm, April 20, 2010, 08:42:47 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

BeadyEm

Hi,

I have recently purchased some Clockwork CIM but I am having problems getting the colour to come out right.  I managed it once on my HH but I have now upgraded to a Bobcat and am  having a few teething problems.  Any suggestions of what I might be doing wrong?  It usually comes out mostly clear with an orangy-red core.

Thanks

Emma

hollergrafik

its a striker, make your bead and it will be mostly clear, let it cool a bit then waft it through the top of the flame, the orange will appear.

BeadyEm

Thanks!  Had another go this morning and now have two fab orange beads! ;D

hollergrafik

Glad it worked for you.

jammie

Ah, didnt realise this either, mine went a sort of swrirly opal orange, quite nice, I must have part struck it.  :)

Dragonfire Glass

You can get some nice results by inadvertently part striking red & oranges - useful when I'm a Fyrebird  ;D